Electron diffraction study of a high-temperature diamond-like silicon ferromagnet with the self-organized superlattice distribution of manganese impurity
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-02-01 |
| Journal | Journal of Experimental and Theoretical Physics Letters |
| Authors | Е. С. Демидов, Vladimir V. Podolskii, В. П. Лесников, Е. Д. Павлова, А. И. Бобров |
| Institutions | Yaroslav-the-Wise Novgorod State University |
| Citations | 4 |
Abstract
Section titled “Abstract”New data on the structure of the diluted magnetic semiconductor Si:Mn with the Curie point to 500 K synthesized by the laser method have been presented. High-resolution electron microscopy and diffraction in the directions 〈110〉 and 〈100〉 of epitaxial layers of the diluted magnetic semiconductor Si:15% Mn with the elimination of the contribution from the GaAs substrate and interface have been applied. It has been established that the diluted magnetic semiconductor Si:Mn is a previously unknown compound with the variable composition Si3 − x Mn x (0 < x < 1), single-phase diamond-like structure, high crystal perfection, and self-organized formation of the superlattice structure with the period of the triple distance between the nearest (110) atomic layers and the interval between the (110) layers doped with Mn atoms and oriented along the growth direction of the Si:Mn film. The layers Si:15% Mn (or Si2.5Mn0.5) consist of 15- to 50-nm blocks with the mutually perpendicular orientations of the superlattice modulations. Manganese atoms in the (110) layers doped with this impurity are located in the form of single-atom stripes, which alternate with the silicon single-atom stripes in agreement with the X-ray spectral analysis and ferromagnetic resonance data. The ferromagnetism of Si3 − x Mn x is associated with a specific feature of the impurity band.