High‐Pressure Synthesis of Boron‐Doped Ultrasmall Diamonds from an Organic Compound
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-08-18 |
| Journal | Advanced Materials |
| Authors | Е. А. Екимов, Oleg S. Kudryavtsev, А.А. Khomich, Oleg I. Lebedev, Tatiana A. Dolenko |
| Institutions | Centre National de la Recherche Scientifique, National Research Nuclear University MEPhI |
| Citations | 64 |
Abstract
Section titled “Abstract”The first application of the high-pressure-high-temperature (HPHT) technique for direct production of doped ultrasmall diamonds starting from a one-component organic precursor is reported. Heavily boron-doped diamond nanoparticles with a size below 10 nm are produced by HPHT treatment of 9-borabicyclo [3,3,1]nonane dimer molecules.