The use of thin diamond films in fiber-optic low-coherence interferometers

MetadataDetails
Publication Date2016-01-21
JournalIOP Conference Series Materials Science and Engineering
AuthorsD. Milewska, Katarzyna Karpieńko
InstitutionsGdańsk University of Technology
Citations1

In this paper we present the use of thin diamond films in fiber-optic low-coherence interferometers. Two kinds of diamond surfaces were used: undoped diamond film and boron- doped diamond film. They were deposited on glass plates as well as silicon layers. A conventionally used mirror was used as a reference layer. Diamond films were deposited using Microwave Plasma Enhanced Chemical Vapour Deposition (μPE CVD) system. Measurements were performed using two superluminescent diodes (SLD) with wavelengths of 1300 mm and 1550 mm. The optimal conditions for each layers were examined: the required wavelength of the light source and the length of Fabry-Perot interferometer cavity. Metrological parameters of Fabry-Perot interferometer with different mirrors were compared. The presented thin diamond films may be an interesting alternative to the commonly used reflective surfaces.