A diamond 14 MeV neutron energy spectrometer with high energy resolution

MetadataDetails
Publication Date2016-02-01
JournalReview of Scientific Instruments
AuthorsTakehiro Shimaoka, Junichi H. Kaneko, Kentaro Ochiai, Masakatsu Tsubota, Hiroaki Shimmyo
InstitutionsNational Institute of Advanced Industrial Science and Technology, Japan Atomic Energy Agency
Citations27
AnalysisFull AI Review Included
  • Objective: Develop a high-resolution 14 MeV neutron energy spectrometer using CVD single-crystal diamond (SCD) to measure deuterium-tritium (DT) plasma ion temperatures.
  • Material Innovation: Self-standing SCD detector fabricated via a specialized lift-off method, eliminating substrate-induced background noise.
  • Performance Breakthrough: Achieved 1.5% high energy resolution for the 12C(n, α)9Be reaction at a 100° measurement angle.
  • Record-Setting Purity: Intrinsic energy resolution (excluding target and circuit noise) reached 0.79%, the best reported for any diamond neutron detector to date.
  • Harsh Environment Stability: Confirmed radiation hardness up to 2 × 1014 neutrons/cm2, suitable for ITER-class fusion reactor diagnostics.
  • Compact Form Factor: Detector active volume of just 2.5 × 2.5 × 0.13 mm3 enables spatially resolved measurements impossible with meter-scale magnetic proton recoil (MPR) or ToF systems.
  • Diagnostic Gap Solved: No competing spectrometer had achieved < 1.0% energy resolution prior to this work, opening the door to precise neutron transport code validation.
ParameterValueUnitContext
Neutron Energy14MeVDT fusion neutron peak
Measurement Angle100°Relative to deuteron beam line
High Energy Resolution1.5%Including target, scattering, and circuit contributions
Intrinsic Energy Resolution0.79%Excluding neutron scattering/slowing and electronics noise
Theoretical Intrinsic Limit0.47%Calculated theoretical floor
Neutron Energy Spread (Calculated vs. Measured)0.6%Propagation of error difference
Detector Active Volume2.5 × 2.5 × 0.13mm3Ideal for ITER 100 ms plasma measurements
Theoretical Detection Efficiency1.0 × 10−5count/(unit neutron flux)For the specified active volume
Diamond Bandgap5.5eVEnables solar-blind, high-temp operation
Maximum Measurable Ion Temperature50keVThreshold for competing reactions
Radiation Hardness Threshold2 × 1014neutrons/cm214 MeV neutrons, stable spectra confirmed
Silicon Detector Damage Threshold1011 - 1012neutrons/cm2Baseline for comparison (100× lower than diamond)
Beam Line Distance30 - 56cmTritide titanium target to detector
Tested Angles95, 100, 110°Angle sweep at FNS beam line
  • Crystal Growth: Single-crystal CVD diamond produced via the lift-off method to obtain free-standing, substrate-free films.
  • Detector Fabrication: Self-standing SCD processed into a functional radiation detector with electrical contacts.
  • Test Facility: Response function measurements conducted at the Fusion Neutronics Source (FNS), 80° beam line, Japan Atomic Energy Agency.
  • Neutron Source: Tritide titanium target bombarded with a deuteron beam to generate 14 MeV neutrons via the D-T reaction.
  • Reaction Channel: 12C(n, α)9Be direct reaction used for energy spectroscopy; no competing reactions below 1 MeV of the peak.
  • Angular Optimization: Energy resolution characterized across 95°, 100°, and 110° detector positions; 100° yielded optimal results.
  • Resolution Deconvolution: Intrinsic resolution isolated by subtracting contributions from neutron scattering, target slowing, and electronic circuit noise.
  • Future Target: Intrinsic resolution goal of ~0.4% via improved electron charge collection efficiency.
  • Applicable Materials: This research requires optical/electronic grade Single Crystal Diamond (SCD) with ultra-low defect density and high charge carrier mobility. 6CCVD supplies SCD films in thicknesses from 0.1 µm to 500 µm, suitable for the 130 µm active volume demonstrated here as well as thinner membrane configurations for next-generation designs.
  • Substrate-Free Delivery: 6CCVD’s capability to deliver free-standing, self-supported SCD plates directly addresses the lift-off process central to this paper, removing the need for researchers to perform risky chemical etching on their own substrates.
  • Custom Dimensions: Detector active areas in the paper (2.5 × 2.5 mm) fall well within 6CCVD’s custom sizing range. We support plates and wafers up to 125 mm (PCD) and offer laser cutting for precise SCD geometries tailored to your experimental chamber.
  • Metalization Options: Charge-collection electrodes are critical for charge collection efficiency (the limiting factor for pushing resolution below 0.4%). 6CCVD’s in-house metalization services (Au, Pt, Pd, Ti, W, Cu) enable optimized ohmic or Schottky contact schemes for SCD detectors. Ti/Pt/Au stack metallization is readily available for stable, low-leakage contacts.
  • Polishing Quality: Surface preparation directly impacts charge collection and spectral resolution. 6CCVD provides SCD polishing to Ra < 1 nm, minimizing surface trap states that degrade detector performance.
  • Radiation-Hard Variants: For extended fusion diagnostics campaigns, Boron-Doped Diamond (BDD) and high-purity PCD options are available for comparative studies or backup detector channels.
  • Engineering Support: 6CCVD’s in-house PhD engineering team can assist with material selection, electrode geometry, and thickness optimization for plasma diagnostics, neutron spectrometry, and fusion reactor instrumentation projects. We routinely consult on charge transport characterization and detector prototyping.
  • Global Logistics: Researchers worldwide can receive materials via global shipping (DDU default, DDP available) to keep timelines on schedule for facility beam-time allocations.

For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

A self-standing single-crystal chemical vapor deposited diamond was obtained using lift-off method. It was fabricated into a radiation detector and response function measurements for 14 MeV neutrons were taken at the fusion neutronics source. 1.5% of high energy resolution was obtained by using the (12)C(n, α)(9)Be reaction at an angle of 100° with the deuteron beam line. The intrinsic energy resolution, excluding energy spreading caused by neutron scattering, slowing in the target and circuit noises was 0.79%, which was also the best resolution of the diamond detector ever reported.