Fluorescent nanodiamonds and their use in biomedical research
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2016-03-15 |
| Journal | Proceedings of SPIE, the International Society for Optical Engineering/Proceedings of SPIE |
| Authors | Lorena P. SuarezāKelly, Isaac V. Rampersaud, Charles Moritz, Amanda R. Campbell, Zhiwei Hu |
| Institutions | King Abdulaziz City for Science and Technology, Columbus NanoWorks (United States) |
| Citations | 5 |
Abstract
Section titled āAbstractāNanodiamonds containing color-centers produce non-quenching fluorescence that is easily detected. This makes them useful for cellular, proteomic and genomic applications. However, fluorescent nanodiamonds have yet to become popular in the biomedical research community as labeling reagents. We discuss production of nanodiamonds with distinct color-centers and assess their biocompatibility and techniques for bioconjugation. Fluorescent diamonds were fabricated by electron irradiation of high-pressure, high-temperature micron-sized diamonds which generated diamonds with vacancy-related defects (V). These diamonds were annealed to create nitrogen vacancy (NV)-centers then following a milling step were fractionated into nanoparticle sizes of 30, 60, and 95 nm. Optical characterization of Vand NV-center diamonds demonstrated fluorescence in two distinct green and red channels, respectively. <i>In vitro</i> studies demonstrated that these nanodiamonds are biocompatible and readily taken up by murine macrophage cells. Quantification of NV-center nanodiamond uptake by flow cytometry, showed that uptake was independent of nanodiamond size. Confocal microscopy demonstrated that NV-center nanodiamonds accumulate within the cytoplasm of these cells. NV-center nanodiamonds were then conjugated with streptavidin using a short polyethylene chain as linker. Conjugation was confirmed via a catalytic assay employing biotinylated-horseradish peroxidase. We present a technique for large-scale production of biocompatible conjugated V- or NV-center nanodiamonds. Functional testing is essential for standardization of fluorescent nanodiamond bioconjugates and quality control. Large-scale production of bioconjugated fluorescent nanodiamonds is crucial to their development as novel tools for biological and medical applications.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2007 - Optical centres produced in diamond by radiation damage.