Double-Layer 3D Macro–Mesoporous Metal Oxide Modified Boron-Doped Diamond with Enhanced Photoelectrochemical Performance
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2016-04-22 |
| Journal | ACS Applied Materials & Interfaces |
| Authors | Jiaqi Fan, Huijie Shi, Hanshuang Xiao, Guohua Zhao |
| Institutions | Tongji University |
| Citations | 57 |
Abstract
Section titled “Abstract”In this work, a TiO<sub>2</sub>/Sb-doped SnO<sub>2</sub> electrode was prepared on the boron-doped diamond (BDD) substrate with double-layer three-dimensional macro-mesoporous (DL3DOM-m) structure, using the polystyrene sphere (PS) vertical deposition method. The as-prepared DL3DOM-m TiO<sub>2</sub>/SnO<sub>2</sub>/BDD was employed for organic contaminant removal, showing excellent photoelectrocatalytic performance. SEM, XRD and XPS indicated that DL3DOM-m electrode possessed a 3D macroporous layered framework with uniform pore size (about 400 nm), nanosized particles (4.5-5.8 nm), and high electroactive surface area (3-fold more than that of BDD). SA-XRD indicated the backbone of DL3DOM-m electrode had mesoporous structure. It was found that the as-prepared electrode exhibited remarkable electrocatalytic activity, high photocurrent and outstanding absorption capability (91.0 μg cm<sup>-2</sup>). Furthermore, bisphenol A (BPA) was completely decomposed after 3 h of reaction applying DL3DOM-m electrode as photoanode, and that on BDD was only 58.9%. It indicated that the modified electrode had great potential to be used in practical water treatment with high photoelectrochemical performance.