Section titled âAbstractâThe structural features of gallium nitride polycrystalline coating formed on a silicon oxide substrate have been considered. It has been shown experimentally that as crystals grow, not only the surface morphology, but crystalline structure and electrophysical parameters of crystals change also. The topography of crystals surfaces at the initial stage of the coating deposition has been found to form due to a diffusion mass transfer.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 1988 - Spravochnik po electrotekhnicheskim materialam
- 2008 - Fizicheskaya elektronika i electronnye pribory: Uchebnoe posobie