Skip to content

Using Si-doped diamond plate of sandwich type for spatial profiling of laser beam

MetadataDetails
Publication Date2016-12-20
JournalLaser Physics Letters
AuthorsV. A. Shershulin, S R Samoylenko, Vadim Sedov, Oleg S. Kudryavtsev, V.G. Ralchenko
InstitutionsRussian Academy of Sciences, National Research Nuclear University MEPhI
Citations2

We demonstrated a laser beam profiling method based on imaging of the laser induced photoluminescence of a transparent single-crystal diamond plate. The luminescence at 738 nm is caused by silicon-vacancy color centers formed in the epitaxial diamond film by its doping with Si during CVD growth of the film. The on-line beam monitor was tested for a cw laser emitting at 660 nm wavelength.