SnowPure Water Technologies earns Presidential “E” award for exports

MetadataDetails
Publication Date2017-05-01
JournalFiltration Industry Analyst
Authors

This chapter gives a brief review of recent developments on the applications of boron-doped diamond (BDD) electrodes. Specifically, electrochemical applications of BDD electrodes for water treatment, ozone generation, organic synthesis, and electrochemical analysis. Additionally several recent examples of recent developments for electrochemical analysis are introduced.