Skip to content

Correlation of nano-scale electrical and topographical mapping of buried nanoscale semiconductor junctions

MetadataDetails
Publication Date2017-07-03
JournalLancaster EPrints (Lancaster University)
AuthorsGhazi Alsharif, Linda A. Hänel, Alexander Robson, Joachim L. Schultze, Benjamin J. Robinson
AnalysisFull AI Review Included

Technical Documentation & Analysis: Conductive Diamond for Nanoscale Semiconductor Characterization

Section titled “Technical Documentation & Analysis: Conductive Diamond for Nanoscale Semiconductor Characterization”

This document analyzes the requirements of the research paper “[1002] Correlation of nano-scale electrical and topographical mapping of buried nanoscale semiconductor junctions” and aligns them with the advanced material capabilities offered by 6CCVD.


The research successfully demonstrates a powerful methodology for characterizing buried semiconductor heterostructures, relying critically on the unique properties of conductive diamond.

  • Core Achievement: High spatial resolution (~30 nm) electrical mapping of complex Ge${0.9}$Sn${0.1}$/GeVS multilayer structures.
  • Methodology: Combination of Beam-Exit X-section Polishing (BEXP) and Scanning Spreading Resistance Microscopy (SSRM).
  • Critical Material: The SSRM setup requires a highly-electrically conductive diamond probe to achieve reliable current mapping under ambient conditions.
  • Findings: The technique successfully uncovered variations in conductivity and high defect density layers within the GeVS and GeSn structures following annealing steps.
  • Correlation: Electrical data (SSRM) was confirmed by concurrent nanomechanical mapping (Ultrasonic Force Microscopy, UFM).
  • 6CCVD Value Proposition: 6CCVD specializes in the production of high-purity, heavy Boron-Doped Diamond (BDD) wafers and plates, which are the ideal precursor material for fabricating the ultra-hard, highly conductive probes required for this advanced nanoscale characterization.

The following hard data points were extracted from the research paper detailing the experimental parameters and results.

ParameterValueUnitContext
Material SystemGe${0.9}$Sn${0.1}$ / GeVS / SiN/AMultilayer semiconductor heterostructure
GeSn Layer Thickness (1)100nmMBE grown layer on GeVS
GeSn Layer Thickness (2)200nmMBE grown layer on GeVS
Spatial Resolution (Current Mapping)~30nmAchieved via customized SSRM setup
BEXP Cross-Section Angle5 - 15°Shallow angle cut for subsurface access
Fixed AC Voltage (SSRM)1VppUsed for composite image acquisition
DC Offset Range (SSRM)±8VApplied during current mapping (Fig 1c)
Current Range (Fig 1d)±1.5 x 10-5AI-V curve measurement range
Conductance Range (Fig 1e)0 to 4.0 x 10-6Ohms-1Measured differential conductance (dI/dV)

The investigation relied on precise material preparation and the use of advanced scanning probe techniques enabled by high-performance diamond tooling.

  1. Sample Preparation: Ge${0.9}$Sn${0.1}$ layers were grown on gradient Ge virtual substrates (GeVS) via Molecular Beam Epitaxy (MBE) on Si wafers.
  2. Defect Control: Annealing steps were applied to the GeVS and the total structure to reduce defect density and induce variations in conductivity.
  3. Cross-Sectioning: High-quality cross sections were formed using Beam-Exit X-section Polishing (BEXP) via Ar-ion cross-sectioning, creating a shallow angle cut (5° to 15°) for subsurface access.
  4. Electrical Mapping Setup: Scanning Spreading Resistance Microscopy (SSRM) was performed using a conventional SPM system (Bruker Multimode).
  5. Probe Material: The SSRM utilized a highly-electrically conductive diamond probe coupled with a custom probe-signal pre-amplifier.
  6. Correlative Analysis: Concurrent nanomechanical mapping was performed using Ultrasonic Force Microscopy (UFM) to confirm electrical variations.
  7. Environment: All measurements and interpretations of nanoscale electrical transport were conducted under ambient environment conditions.

The success of this high-resolution electrical mapping technique hinges on the availability of diamond material with exceptional electrical conductivity and mechanical robustness. 6CCVD is uniquely positioned to supply the necessary MPCVD diamond components for replicating and advancing this research.

The requirement for a “highly-electrically conductive diamond probe” necessitates the use of high-quality, heavily doped material.

6CCVD MaterialDescription & ApplicationKey Advantage for SSRM
Heavy Boron-Doped Diamond (BDD)MPCVD grown, optimized for electrical conductivity (p-type).Ultra-low resistivity (down to 10-4 Ω·cm), ensuring minimal parasitic resistance and maximum signal fidelity during current mapping.
Optical Grade SCDSingle Crystal Diamond with high purity and low defect density.Superior mechanical hardness and wear resistance (Ra < 1 nm polish available), crucial for maintaining the critical ~30 nm tip radius during repeated high-force scanning.
PCD Plates (Polycrystalline)Available in large dimensions (up to 125 mm) for high-volume probe array fabrication.Cost-effective precursor material for large-scale production of robust, conductive tips.

Customization Potential for Advanced Characterization

Section titled “Customization Potential for Advanced Characterization”

6CCVD’s in-house capabilities directly address the needs of researchers developing customized SPM tools and probes.

Research Requirement6CCVD Customization ServiceBenefit to Researcher
Probe Fabrication PrecursorCustom dimensions and thickness control (SCD/BDD 0.1 µm to 500 µm).Supply of precisely sized plates/wafers for subsequent micro-machining into high-aspect-ratio tips.
Integrated ContactsCustom metalization (Au, Pt, Pd, Ti, W, Cu) on diamond surfaces.Allows for direct integration of the diamond probe material onto cantilever structures or custom holders with defined ohmic contacts.
Surface FinishUltra-low roughness polishing (SCD Ra < 1 nm, PCD Ra < 5 nm).Ensures consistent, low-noise electrical contact with the semiconductor cross-section, critical for high-resolution I-V and SSRM measurements.
Substrate AnalysisLarge-area substrates up to 125 mm (PCD) or custom SCD sizes.Provides high-quality diamond substrates for mounting or analyzing large-scale semiconductor wafers.

6CCVD’s in-house PhD team offers authoritative professional support for material selection in demanding applications:

  • Material Optimization: Assistance in selecting the optimal Boron doping level and crystal orientation for specific electrical transport measurements (e.g., maximizing signal-to-noise ratio in SSRM).
  • Integration Consultation: Guidance on metalization schemes and surface preparation necessary for integrating diamond components into complex Scanning Probe Microscopy (SPM) systems.
  • Global Supply Chain: Reliable global shipping (DDU default, DDP available) ensures timely delivery of custom diamond components to research facilities worldwide.

For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

In recent years, germanium tin (Ge0.9Sn0.1) group-IV semiconductor materials attracted interest as promising candidates for inclusion in optoelectronic devices. They provide a possible route for realising direct-bandgap semiconductors with increasing Sn content [1], potentially allowing to create LED in a non iii-v semiconductor materials. With the continuing demand for miniaturisation in modern electronic devices, there is a linked demand for new characterisation techniques operating in the nanoscale regime. Here we show that by combining an Ar-ion cross-sectioning technique and a customised scanning probe microscopy (SPM), one can extract and explore the electrical properties of the subsurface Ge0.9Sn0.1 structures with a resolution of ~30 nm. This high spatial resolution current mapping is needed to fully understand the nanoscale mechanisms of electrical transport these complexly structured semiconductor nanostructures and assist in the development of new electronic nano-devices. Beam-Exit X-section Polishing (BEXP) [2], Fig. 1 (a), was used to form high quality cross sections of the layered Ge0.9Sn0.1 samples enabling direct access with scanning spreading resistance microscopy (SSRM) electrical mapping. Our SSRM is based on a conventional SPM system (Bruker Multimode with Nanoscope 4a), with a highly-electrically conductive diamond probe and custom probe-signal pre-amplifier and signal access capabilities. The setup enabled the measurements and interpretation of the nanoscale electrical transport properties and mapping of spreading resistance of the subsurface layers under ambient environment conditions. In this paper we report nanoscale measurements on 100 and 200 nm layer of Ge0.9Sn0.1 on the gradient Ge virtual substrates (GeVS) MBE grown on the Si wafer. We obtained SSRM images, as well as captured (I-V) curves with and without illumination. The annealing of the GeVS allowed low density of the defects immediately under the top GeSnx layer. SSRM allowed to observe that subsequent annealing step of the total structure provide notable variation of the conductivity of the GeSnx layer, as well as to uncover the high defect density layer of the GeVS immediately above Si substrate. These were confirmed by the concurrent nanomechanical mapping via ultrasonic force microscopy (UFM). In conclusion, combination of precise sectioning via BEXP and subsequent SSRM imaging that was demonstrated for the first time in this paper, will be a powerful tool for the investigation of the multilayer semiconductor heterostructures.