The field emission from nanocrystalline diamond film coated silicon carbide microstructured cathode
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2017-07-01 |
| Authors | В. В. Лучинин, Vladimir A. Golubkov, Alexey Ivanov, Vladimir A. Ilyin, С. А. Богданов |
| Institutions | Institute of Applied Physics, Saint Petersburg State Electrotechnical University |
Abstract
Section titled “Abstract”Silicon carbide field emission arrays coated with two different type of nanocrystalline diamond thin film: undoped and highly boron-doped are compared. The last one shows two times lower electric field threshold for electron emission.