The doping level of boron-doped diamond electrodes affects the voltammetric sensing of uric acid

MetadataDetails
Publication Date2018-01-01
JournalAnalytical Methods
AuthorsKristína Cinková, Kristína Kianičková, Dalibor Stanković, Marián Vojs, Marián Marton
InstitutionsCzech Academy of Sciences, Institute of Analytical Chemistry, Slovak University of Technology in Bratislava
Citations42

In this work, the electrochemical oxidation and subsequent determination of uric acid was investigated using boron-doped diamond electrodes with various B/C ratios (0-2000 ppm).