Three-dimensional Graphite Electrodes Buried in sc-CVD Diamond - Investigation with electrons and proton micro-beam,
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | Iris (Roma Tre University) |
| Authors | M. Girolami, S. Salvatori, P. Oliva, A. Bellucci, D.M. Trucchi |
Abstract
Section titled āAbstractāA detailed characterization under 90Sr β-particles and 4.5 MeV protons micro-beam of a single-crystal CVD diamond-based three-dimensional detector with surface and buried graphite electrodes is presented. Pillar contacts, 300 μm long and 30 μm diameter, were fabricated by using a femtosecond laser operating at 1030 nm wavelength and 400 fs pulse duration. Charge collected under 90Sr β-particles was measured in front and back irradiation conditions, pointing out that the pillars contribute to the charge collection. Charge collection efficiency (CCE) was measured to be up to 94% under proton beam irradiation. Results of a comprehensive study, including crossed-polarizers imaging, numerical simulation of the electric field distribution, and proton mapping, show that CCE is not affected from the stress induced by the pillar fabrication, and that the electric field strength is high enough to partially compensate for carrier recombination in the defected regions surrounding the pillars.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal Sourceā- DOI: None