Versatile multicolor nanodiamond probes for intracellular imaging and targeted labeling
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | Journal of Materials Chemistry B |
| Authors | Kerem Bray, Leonard Cheung, Khondker R. Hossain, Igor Aharonovich, Stella M. Valenzuela |
| Institutions | University of Technology Sydney |
| Citations | 18 |
Abstract
Section titled āAbstractāWe report on the first demonstration of FNDs containing either silicon or nitrogen vacancy color centers for multi-color bio-imaging.