Cu doped diamond - Effect of charge state and defect aggregation on spin interactions in a 3d transition metal doped wide band-gap semiconductor
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-05-11 |
| Journal | Journal of Applied Physics |
| Authors | E. M. Benecha, E. B. Lombardi |
| Institutions | University of South Africa |
| Citations | 6 |
Abstract
Section titled āAbstractāWe present a first principles study of Cu in diamond using DFT+U electronic structure methods, by carefully considering the impact of co-doping, charge state, and Fermi level position on its stability, lattice location, spin states, and electronic properties. We show that the energetic stability and spin states of Cu are strongly dependent on the Fermi level position and the type of diamond co-doping, with Cu being energetically more favorable in n-type or p-type co-doped diamond compared to intrinsic diamond. Since Cu has been predicted to order magnetically in a number of other wide band-gap semiconductors, we have also evaluated this possibility for Cu doped diamond. We show that while Cu exhibits strong spin interactions at specific interatomic separations in diamond, a detailed consideration of the impact of Fermi level position and Cu aggregation precludes magnetic ordering, with Cu forming non-magnetic, antiferromagnetic, or paramagnetic clusters. These results have important implications in the understanding of the properties of transition metal dopants in diamond for device applications.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2009 - CVD Diamond for Electronic Devices and Sensors