Abstract
Section titled “Abstract”Purpose The purpose of this study is to investigate the mechanical and tribological properties of the synthetic diamond coatings deposited on WC-Co cutting tools for their prospective applications in mechanical industry. In this work, the concept of nanocrystalline diamond, microcrystalline diamond and multilayer-diamond coating systems were proposed and deposited on WC-Co substrates with the top-layer nanocrystallinity, optimum thickness and interfacial adhesion strength for load-bearing tribological and machining applications. Also, the overall mechanical and tribological properties of all synthetic diamond coatings were compared for the purpose of selecting a suitable type of protective layer used on the surfaces of WC-Co cutting tools or mechanical dies. Design/methodology/approach Smooth and adhesive single layered and multilayered synthetic deposited on chemically etched cemented tungsten carbide (WC-Co) substrates using predetermined process parameters in hot filament chemical vapor deposition (HFCVD) method. A comparison has been documented between diamond coatings having different nature and architecture for the purpose of studying their mechanical and tribological characteristics. The friction characteristics were studied experimentally using ball-on-disc type linear reciprocating micro-tribometer under the influence of varying load conditions and within dry sliding conditions. Nanoindentation tests were conducted on each diamond coating using Berkovich nanoindenter for the measurement of their hardness and elastic modulus values. Also, the wear characteristics of all sliding bodies were studied under varying load conditions using cumulative weight loss and density method. Findings Depositing any type of diamond coating on the cemented carbide tool insert increases its all mechanical and tribological characteristics. When using boron-doping onto the top-layer surface of diamond coatings decrease slightly their mechanical properties but increases the tribological characteristics. Present analysis reveals that friction coefficient of all diamond-coated WC-Co substrates decreases with the increase of normal load. Therefore, maintaining an appropriate level of normal load, sliding time, sliding distance, atmospheric conditions and type of diamond coating, the friction coefficient may be kept to some lower value to improve mechanical processes. Originality/value As the single layered synthetic diamond coatings have not given the full requirements of mechanical and tribological properties when deposited on cutting tools. Therefore, the multilayered diamond coatings were proposed and developed to enhance the interfacial integrity of the nanocrystalline and microcrystalline layers (by eliminating the sharp interface) as well as increasing the hardness of tungsten carbide substrate. However, when using boron doping onto the top-layer surface of diamond, coatings decreases slightly their mechanical characteristics but also decreases the value of friction coefficient.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2007 - Nano to micrometric HFCVD diamond adhesion strength to Si3N4
- 1983 - Experimental investigation of the effect of system rigidity on wear and friction-induced vibrations [Crossref]
- 1984 - Interact ions among friction, wear, and system stiffness-part 1: effect of normal load and system stiffness
- 2011 - The effect of sliding speed and normal load on friction and wear property of aluminum
- 1998 - Adhesion and debonding of multilayer thin film structures [Crossref]
- 2013 - Growth and characterization of integrated nano- and microcrystalline dual layer composite diamond coatings on WC-Co substrates [Crossref]
- 1999 - Tribological properties of nanocrystalline diamond films
- 2002 - Diamond and hard carbon films for microelectromechanical systems (MEMS)-a nanotribological study
- 2015 - Preparation and cutting performance of boron-doped diamond coating on cemented carbide cutting tools with high cobalt content
- 2016 - Effect of CVD-diamond coatings on the tribological performance of cemented tungsten carbide substrates