Experimental Simulation of a Diamond Betavoltaic Battery
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-08-01 |
| Journal | Technical Physics Letters |
| Authors | V. N. Amosov, V. N. Babichev, N. A. Dyatko, S. A. Meshchaninov, A. F. Palā |
| Institutions | Troitsk Institute for Innovation and Fusion Research |
| Citations | 4 |
Abstract
Section titled āAbstractāDiamond single-crystal Schottky barrier mip-structures (metal-intrinsic diamond-p-doped diamond) with dimensions of 3 Ć 3 and 4.1 Ć 4.28 mm are fabricated on the basis of HTHP p-diamond and CVD i-diamond. The betavoltaic characteristics of the diamond structures are studied using a wide-aperture electron beam with an initial energy of 110 keV, partially scattered on the way to a converter by a 14-μm-thick aluminum layer and a 17-mm-thick air layer. The maximum generated power reached 2.18 mW (41 mW/cm2) with a conversion efficiency of 2-3%.