Observation of the linewidth broadening of single spins in diamond nanoparticles in aqueous fluid and its relation to the rotational Brownian motion
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-09-27 |
| Journal | Scientific Reports |
| Authors | Masazumi Fujiwara, Yutaka Shikano, Ryuta Tsukahara, Shinichi Shikata, Hideki Hashimoto |
| Institutions | Keio University, Institute for Molecular Science |
| Citations | 12 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Core Innovation: First experimental confirmation that the Optically Detected Magnetic Resonance (ODMR) linewidth of single Nitrogen-Vacancy (NV) centers broadens in direct proportion to the rotational diffusion constant of the host nanodiamond.
- Key Achievement: Measured a precise 1.8 MHz linewidth broadening (FWHM) when nanodiamonds detached from a substrate in an aqueous buffer (pH 9.1), aligning perfectly with the Einstein-Smoluchowski relation for an 11.4 nm particle diameter.
- Methodology: Used a custom perfusion chamber combined with confocal fluorescence microscopy and gated continuous-wave (cw) ODMR to monitor single NV centers transitioning from a fixed to a free-floating state.
- Technical Validation: Confirmed the signal source was rotational motion, not power fluctuations, by analyzing laser saturation intensity (0.34 mW) and microwave power dependencies.
- Quantum Sensing Application: Provides a novel pathway to measure the rotational Brownian motion of single nanoparticles below the optical diffraction limit, paving the way for nanofluidics and single-protein tracking.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Nanodiamond Median Size | 25 | nm | Commercial source (Microdiamant, MSY 0-0.05) |
| Target Particle Diameter | 11.4 | nm | Calculated via Einstein-Smoluchowski relation |
| Baseline ODMR Linewidth | 12.2 (± 0.4) | MHz | FWHM of major peak when fixed to coverslip |
| Detached ODMR Linewidth | ~14.0 | MHz | FWHM broadened due to rotational Brownian motion |
| Linewidth Broadening (ΔFWHM) | 1.8 | MHz | Difference between fixed and fluctuating states |
| Major Peak Position | 2.8784 (± 0.0001) | GHz | Zero-field splitting (ZFS) of NV ground state |
| Minor Peak Position | 2.9036 (± 0.0011) | GHz | Intrinsic strain splitting of magnetic sublevels |
| Laser Excitation Wavelength | 532 | nm | Continuous wave (cw) green laser |
| Laser Excitation Intensity | 94 | kW·cm-2 | Equivalent to 250 µW |
| Laser Saturation Intensity | 0.34 | mW | Calculated from photon count saturation |
| Microwave Excitation Power | 35 | dBm (3.2 W) | Input power to the linear antenna |
| APD Gate Width | 200 | µs | Gated photon counting for ODMR contrast |
| APD Repetition Rate | 2 | kHz | Gating frequency for microwave ON/OFF |
| Flow Rate | 80 | µL · min-1 | Continuous buffer circulation to prevent photothermal accumulation |
| pH Transition Range | 7.5 → 9.9 → 9.1 | pH | 0.1 M sodium carbonate buffer with 5% HCl |
| Spin Count Rate | ~150 | kcps | Average fluorescence count of single NV centers |
| g(2)(0) Value | 0.16 | (unitless) | Antibunching dip (zero-delay time, t0 = 47 ns) |
| Metastable State Lifetime (τ1) | 11 | ns | Population exchange parameter |
| Bunching Shoulder (τ2) | 166 | ns | Fluorescence correlation lifetime |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Cleaned coverslips were spin-coated with a purified nanodiamond suspension (centrifuged 5x at 14,300 RCF to remove sp2 soot) and characterized via Atomic Force Microscopy (AFM).
- Perfusion Chamber Fabrication: An acrylic spacer (~4 mm height) with inlet/outlet tubes was UV-resin bonded to the sample. A 25 µm thin copper wire was positioned as a microwave linear antenna and soldered to SMA connectors.
- Liquid Handling: Distilled water was initially injected, followed by a stepwise pH transition (7.5 → 8.2 → 9.1 → 9.9 → 9.1) utilizing a 0.1 M sodium carbonate buffer and HCl.
- Confocal Microscopy: A 3-axis piezo stage scanned a home-built confocal microscope utilizing an oil-immersion objective (NA = 1.4) to achieve single-particle resolution.
- Optical Filtering: A dichroic beam splitter (FF560-FDi01) and long-pass filter (BLP01-561R) isolated the red-shifted NV fluorescence into a single-mode fiber (10 µm core).
- Photon Detection: Fluorescence was routed to a Hanbury-Brown-Twiss (HBT) setup featuring two APDs (SPCM AQRH-14) and a 50:50 beam splitter, or a liquid-nitrogen-cooled CCD spectrometer.
- ODMR Implementation: A microwave source (SMB100A) amplified by 45 dB (ZHL-16W-43+) drove the antenna. An RF switch (ZYSWA-2-50DR-S) and bit pattern generator (PBESR-PRO-300) enabled gated photon counting (200 µs gates, 2 kHz repetition).
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Transitioning this quantum sensing platform from research to robust commercial or biomedical applications requires ultra-high-purity diamond materials. Below is how our manufacturing capabilities align with the requirements of NV-based rotational sensors.
Applicable Materials
Section titled “Applicable Materials”- Optical Grade Single Crystal Diamond (SCD): The foundation of this research relies on isolated NV centers with stable photoluminescence. Our SCD wafers, polished to Ra < 1 nm, provide the ideal lattice structure for hosting NV centers with minimal inhomogeneous strain (critical for resolving the 12.2 MHz vs ~14.0 MHz FWHM distinctions seen in this paper).
- Ultra-Fine Polycrystalline Diamond (PCD) Powder/Suspensions: To replicate the Microdiamant MSY 0-0.05 (25 nm) nanodiamonds used here, custom-engineered PCD nanodiamond suspensions can be tailored with precise particle size distributions.
- Boron-Doped Diamond (BDD): For future iterations aiming to tune the zeta potential and optimize substrate detachment mechanics in fluidic environments, heavy boron-doped PCD offers tunable surface charge properties.
Customization Potential
Section titled “Customization Potential”- Precision Laser Cutting: The paper utilized spin-coating to disperse nanodiamonds. For advanced microfluidic sensor arrays, 6CCVD can provide laser-cut SCD or PCD membranes with custom geometries, allowing researchers to engineer bespoke perfusion chambers and substrates.
- Advanced Metalization: The researchers utilized a bare 25 µm copper wire as a microwave antenna. 6CCVD offers in-house metalization with Au, Pt, Pd, Ti, W, and Cu, enabling the fabrication of patterned microwave waveguides or coplanar resonators directly onto SCD/PCD substrates for stronger, more uniform spin excitation.
- Wafer Dimensions: While this paper used a coverslip, scaling this sensor architecture to integrated quantum chips requires larger surfaces. 6CCVD manufactures plates and wafers up to 125 mm (PCD).
Engineering Support
Section titled “Engineering Support”Developing reliable NV-based nanofluidic sensors requires careful control over NV density, spin coherence, and surface chemistry. The 6CCVD in-house PhD engineering team can assist researchers in selecting the optimal diamond grade, thickness (0.1 µm to 500 µm for SCD/PCD), and surface functionalization to match the specific rotational diffusion timescales of their target nanoparticles.
For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Capturing the fast rotational motion of single nanoparticles has been hindered owing to the difficulty of acquiring directional information under the optical diffraction limit. Here, we report the linewidth broadening of the electron spin resonance of single nitrogen vacancy (NV) centers that matches the rotational diffusion constant of the host nanodiamonds. When nanodiamonds are gradually detached from the substrates that they were fixed to, their optically detected spin resonance peaks are broadened by 1.8 MHz, which corresponds to the rotational diffusion constant of nanoparticles with a diameter of 11.4 nm from the Einstein-Smoluchowski relation.