AuthorsTibor Ižák, Ondrej Szabó, Pavla Štenclová, Štěpán Potocký, Vlastimil Vyskočil
InstitutionsCzech Academy of Sciences, Institute of Physics, Charles University
Citations2

In the present study, we introduce various technological approaches for fabrication of structured boron-doped diamond (BDD) electrodes, i.e., nanocones and nanorods which are used as working electrodes for electrochemical measurements. Structured BDD were realized either by reactive ion etching employing gold nanoclusters as the mask or by thermo-catalytically induced modification of the diamond surface. All samples were characterized in terms of surface morphology (scanning electron microscopy images), chemical composition (Raman spectroscopy) and electrochemical properties (anodic stripping voltammetry).

  1. 2013 - In situ synthesis and properties of reduced graphene oxide/Bi nanocomposites: As an electroactive material for analysis of heavy metals [Crossref]
  2. 2016 - Nanocarbon-based Electrochemical Detection of Heavy Metals [Crossref]
  3. 2012 - Upstream microelectrodialysis for heavy metals detection on boron doped diamond [Crossref]
  4. 2002 - Simultaneous Electrochemical Detection and Determination of Lead and Copper at Boron-Doped Diamond Film Electrodes [Crossref]
  5. 2006 - A comparison of boron-doped diamond thin-film and Hg-coated glassy carbon electrodes for anodic stripping voltammetric determination of heavy metal ions in aqueous media [Crossref]
  6. 2007 - Anodic Stripping Voltammetry of Heavy Metals at Nanocrystalline Boron-Doped Diamond Electrode [Crossref]
  7. 2006 - Detection of trace levels of Pb2+ in tap water at boron-doped diamond electrodes with anodic stripping voltammetry [Crossref]
  8. 2015 - Technological Aspects in Fabrication of Micro- and Nano-Sized Carbon Based Features: Nanorods, Periodical Arrays and Self-Standing Membranes
  9. 2009 - Nanostructuring of diamond films using self-assembled nanoparticles [Crossref]
  10. 2008 - ICP etching of polycrystalline diamonds: Fabrication of diamond nano-tips for AFM cantilevers [Crossref]