Detection of magnetic thin film impurity phases using nitrogen vacancy centers in diamond crystal
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Authors | Andris BÄrziÅÅ”, JÄnis Å mits, Andrejs Petruhins, Johanna RosĆ©n, A. Smiltnieks |
| Institutions | Thinfilm (Sweden), Linkƶping University |
Abstract
Section titled āAbstractāWe demonstrate the possibility to detect magnetic impurity phases in thin films using magnetic field imaging technique based on a layer of nitrogen-vacancy centers in the diamond lattice. We demonstrate results of magnetic field distributions created by impurity phases as well as mechanical defects on the thin film surface.