Electrochemical reduction of CO2 using palladium modified boron-doped diamond electrodes - enhancing the production of CO

MetadataDetails
Publication Date2019-01-01
JournalPhysical Chemistry Chemical Physics
AuthorsPrastika Krisma Jiwanti, Yasuaki Einaga
InstitutionsKeio University, Early Manuscripts Electronic Library
Citations35

Electrochemical reduction of CO<sub>2</sub> produced CO on PdBDD electrode at potential āˆ’1.6 V (<italic>vs.</italic> Ag/AgCl) in NaCl aqueous solution.