Skip to content

Hybrid refractive-diffractive microlenses in glass by focused Xe ion beam

MetadataDetails
Publication Date2019-08-07
JournalJournal of Vacuum Science & Technology B Nanotechnology and Microelectronics Materials Processing Measurement and Phenomena
AuthorsSergey Gorelick, Alex de Marco
InstitutionsARC Centre of Excellence in Advanced Molecular Imaging, Monash University
Citations7

The combination of refractive and diffractive components in a single optical element provides miniaturization of optical systems and enhancement of their performance. Thus, hybrid singlet lenses with diffractive structures added on top of the refractive curved surface were shown to have reduced chromatic and spherical aberration. Optical systems based on such hybrid lenses have reduced dimensions as they require fewer lenses for aberrations-correction. Diffractive elements provide additional possibilities of light manipulation and enable the realization of miniaturized multifocal systems, spectrometers, and other devices. Glass hybrid lenses are typically realized by diamond turning or glass moulding. These techniques, however, are not applicable for the fabrication of lenses in brittle materials or microlenses (hundreds of micrometers in diameter or less). On the other hand, direct writing techniques, such as focused ion beam (FIB) milling (typically Ga), offer a high resolution and flexibility of patterning on curved lens surfaces made of a great variety of materials. The disadvantages of FIB milling are its slow speed and Ga implantation that may alter or degrade the optical performance of fabricated components. FIB systems based on high brightness plasma ion sources provide more than an order of magnitude increase in milling rates with noble gas ions (e.g., Xe) compared with Ga FIBs. Here, the authors demonstrate the feasibility of rapid, direct milling of hybrid refractive-diffractive microlenses in glass using >60 nA of Xe ion current. Microlenses with up to 300-μm diameter were milled and diffraction gratings were realized on top of their curved surfaces. The performance of the lenses was characterized by mapping the transmitted intensity at different positions. Due to the introduction of diffraction gratings on the surface of the lenses, their optical performance is modified with the emergence of additional focal spots spatially separated by distances consistent with the theoretical and simulated values. The results indicate the applicability of the plasma focused ion beam systems for rapid fabrication of high-quality hybrid optical elements directly in hard substrates.

  1. **** - Proc. SPIE [Crossref]
  2. 1992 - Proc. SPIE [Crossref]