Skip to content

The Interface and Mechanical Properties of a CVD Single Crystal Diamond Produced by Multilayered Nitrogen Doping Epitaxial Growth

MetadataDetails
Publication Date2019-08-06
JournalMaterials
AuthorsYun Zhao, Chengming Li, Jinlong Liu, Kang An, Xiongbo Yan
InstitutionsUniversity of Science and Technology Beijing
Citations13

In the present investigation, a nitrogen-doped multilayer homoepitaxial single crystal diamond is synthesized on a high-pressure high temperature (HPHT) Ib-type diamond substrate using the microwave plasma chemical vapor deposition (MPCVD) method. When 0.15 sccm of nitrogen was added in the gas phase, the growth rate of the doped layer was about 1.7 times that of the buffer layer, and large conical and pyramidal features are formed on the surface of the sample. Raman mapping and photoluminescence imaging of the polished cross sectional slice shows a broadband emission, with a characteristic zero phonon line (ZPL) at 575 nm in the doped layers, and large compressive stress was formed in the nitrogen-doped layers. X-ray topography shows that the defects at the interface can induce dislocation. The pyramid feature is formed at the defect, and more nitrogen-related defects are formed in the pyramid region. Thin nitrogen-doped multilayers were successfully prepared, and the thickness of the nitrogen-doped and buffer layers was about 650 nm each. The indentation measurements reveal that the thin nitrogen-doped multilayers are ultra-tough (at least ~22 MPa m1/2), compared to the Ib-type HPHT seed substrate (~8 MPa m1/2) and the unintentionally doped chemical vapor deposition (CVD) single crystal diamond (~14 MPa m1/2).

  1. 2009 - Recent advances in high-growth rate single-crystal CVD diamond [Crossref]
  2. 2018 - Comparison of the quality of single-crystal diamonds grown on two types of seed substrates by MPCVD [Crossref]
  3. 2009 - Composite chemical vapor deposition diamond anvils for high-pressure/high-temperature experiments [Crossref]
  4. 2009 - Enhancing the mechanical properties of single-crystal CVD diamond [Crossref]
  5. 2004 - Ultrahard diamond single crystals from chemical vapor deposition [Crossref]
  6. 2018 - Revealing the formation mechanism of ultrahard nanotwinned diamond from onion carbon [Crossref]
  7. 2014 - Nanotwinned diamond with unprecedented hardness and stability [Crossref]
  8. 1970 - Attempt to design a strong solid [Crossref]
  9. 2007 - On the role of nitrogen in stiffening the diamond structure [Crossref]