Boron‐Doped Diamond - Boron‐Doped Diamond for Hydroxyl Radical and Sulfate Radical Anion Electrogeneration, Transformation, and Voltage‐Free Sustainable Oxidation (Small 48/2019)
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-11-01 |
| Journal | Small |
| Authors | Junzhuo Cai, Tiezheng Niu, Penghui Shi, Guohua Zhao |
| Institutions | Shanghai University of Electric Power, Shanghai Institute of Pollution Control and Ecological Security |
| Citations | 5 |
Abstract
Section titled “Abstract”Boron-doped diamond is perfect for efficient and sustainable oxidation of pollutants with aid of electrochemically generated radicals. In article number 1900153, Penghui Shi, Guohua Zhao, and co-workers provide theoretical and experimental evidence of in-situ generation of SO4•− radicals as well as their oxidation mechanism of pollutants on boron-doped diamond surfaces.