CuMSe for thermoelectric applications
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-01-01 |
| Journal | DR-NTU (Nanyang Technological University) |
| Authors | Quresh Asgarali |
Abstract
Section titled āAbstractāAlthough demand for thermoelectrics may have shown promising advantages due to nanoscale features, thermoelectric materials have paid considerable attention to their ability to convert waste heat to useful electricity. A rebirth in thermoelectric study led to substantial improvements in the thermoelectric merit figure, zT, including materials that had previously been meticulously examined. This study focuses on thermoelectric zT optimization by developing a comprehensive analysis of the electronic structure through amalgamation of optical properties, ab initio computed electronic band structures and electronic / thermoelectric properties. \n \nIn IV-VI semiconductor materials (PbTe,PbSe,PbS), a fluctuating temperature-dependent optical absorption edge is presented which is well associated with the calculated ab initio molecular dynamics output. A higher union temperature of 700, 900 and 1000 K for PbTe, PbSe and PbS is projected, as opposed to previous works involving the merging of primary and secondary bands at 400 K. This disassembly can influence the modeling of electronic properties by providing a tangible value for the valence band and the offset band gap as a function of temperature. \n \nThe alternative thermoelectric material, ZrNiSn, is examined for both its electronic and optical properties. Conversely, the transport properties imply a substantially different band gap, depending on whether the material is p-type or n-type doped. By quantifying and testifying the optical band gap value of 0.13 eV, the inconsistency in the gap computed from the electronic properties can be resolved by associating these assessments with the weighted mobility ratio, A, in narrow gap materials. \n \nDue to its low thermal conductivity and adjustable electrical conductivity, Ternary Cu_2 SnSe_3 material with a diamond-like structure has been fitted as one of the latent thermoelectric materials. In this study, the Cu_2 SnSe_3 powder is produced by the vacuum melting-quenching-annealing-grinding process. Electrical resistance, Seebeck coefficient and thermal conductivity measurement are used for the analysis of thermoelectric properties.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal Sourceā- DOI: None