Skip to content

Theoretical and experimental study of the influence of cation–Eriochrome complexes on the BDD anodic oxidation of Eriochrome Black T solutions

MetadataDetails
Publication Date2020-01-23
JournalElectrochemistry Communications
AuthorsÁmison Rick Lopes da Silva, Alexsandro J. dos Santos, Elisama Vieira dos Santos, Djalma Ribeiro da Silva, Carlos A. Martínez‐Huitle
InstitutionsUniversidade Federal do Rio Grande do Norte
Citations13

It has previously been established during the elimination of Eriochrome Black T (EBT) that water hardness is an important condition that limits the efficacy of electrochemical treatments of azo dye effluent by the electrophilic attack of ·OH radicals, due to the possible formation of calcium and magnesium complexes. This outcome was observed when using the Electro-Fenton (EF) approach, where the use of iron as a catalyst is mandatory; however, the synergistic or antagonistic effects of iron were not considered. For this reason, this communication presents important experimental and theoretical insights (using Density Functional Theory (DFT) and Quantum Theory of Atoms in Molecules (QTAIM)) into the influence of different ions (Ca2+, Mg2+ or Fe2+) on the degradation efficiency of EBT solution using anodic oxidation (AO) with boron-doped diamond (BDD) electrodes. Keywords: Boron-doped diamond, DFT, QTAIM, EBT anodic oxidation, Dye, Hydroxyl radicals