Skip to content

Precision Coating of ta-C Films on Quartz Surfaces

MetadataDetails
Publication Date2020-09-03
AuthorsKotaro Kawai, Yuki Hirata, Hiroki Akasaka, Naoto Ohtake
InstitutionsTokyo Institute of Technology

Abstract Diamond-like carbon (DLC) films have excellent properties such as high hardness, low friction coefficient, high wear resistance, chemical inertness and so on. Because DLC film is considered as an effective coating material to improve their surface properties, this films are used in various applications such as parts for automobiles engines, hard disk surfaces, cutting tools and dies, and so on. DLC films consist of a mixture of sp2 bonded carbon atoms and sp3 bonded carbon atoms. Among them, ta-C film is known as the hardest and strongest film since it mainly consists of sp3 bonded carbon atoms. One of deposition methods to form ta-C is Filtered Cathodic Vacuum Arc (FCVA). The characteristic of this method is that it is possible to remove the droplets and form a high-quality film.. However, even though lots of mechanical components which require ta-C coating have three-dimensionally shapes, it is difficult to coat ta-C film three dimensionally by using FCVA process. At present, researches on 3D deposition of amorphous carbon films on three dimensional components is still insufficient, and investigation reports on the deposition mechanism and characterization of the deposited films are even more limited. In this study, we tried to deposit films on 3D components by the FCVA method and evaluated the microstructure and surface morphologies of films. Although films were coated successfully in the entire surfaces, different properties were showed depending on the location of components. These properties were investigated by Raman spectroscopy and laser microscope.