Secondary Radiation in Microdiamonds with NV Centers
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-11-01 |
| Journal | Crystallography Reports |
| Authors | Š. Š”. ŠŠ¾Ńелик, S. Š. Savinov, V. V. Sychev, Dongxue Bi |
| Institutions | P.N. Lebedev Physical Institute of the Russian Academy of Sciences, Bauman Moscow State Technical University |
| Citations | 2 |
Abstract
Section titled āAbstractāThe regularities in the secondary radiation (fluorescence and Raman) spectra of single diamond microcrystals have been investigated. The Raman spectrum excited by infrared laser radiation exhibits the fundamental diamond mode with a frequency of 1332 cm-1 and a two-phonon band peaking at a frequency of 2615 cm-1. The fluorescence spectra contain zero-phonon lines of NV centers with a pronounced phonon structure.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2001 - Optical Properties of Diamond. A Data Handbook [Crossref]