An efficient, formic acid selective CO2 electrolyzer with a boron-doped diamond cathode

MetadataDetails
Publication Date2021-01-01
JournalSustainable Energy & Fuels
AuthorsJinglun Du, Andrea Fiorani, Yasuaki Einaga
InstitutionsKeio University
Citations16

A diamond electrode-based CO<sub>2</sub> electrolyzer was fabricated. With this electrolyzer, a faradaic efficiency of 96% and electrical-to-chemical energy conversion efficiency of 43% for the production of formic acid can be obtained.