Modification of boron-doped diamond electrodes with gold–palladium nanoparticles for an oxygen sensor
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2021-01-01 |
| Journal | The Analyst |
| Authors | Tribidasari A. Ivandini, Muhammad S. P. Luhur, Munawar Khalil, Yasuaki Einaga |
| Institutions | Keio University, Financial Management Association International |
| Citations | 13 |
Abstract
Section titled “Abstract”Boron-doped diamond modified with gold-palladium nanoparticles (Au@PdNPs) <italic>via</italic> allylamine bridges for oxygen sensors. Exposed gold in Au@PdNPs contributed to the attachment process and palladium enhances the responses of the oxygen reduction reaction.