Principle study of structure, energetics, and electrical properties of Ge-N-vacancy complexes in diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2021-02-18 |
| Journal | Journal of the Optical Society of America B |
| Authors | Xin Tan, Zhixin Liu, Bochen Zhang, Luhua Chen, Xueyuan Wei |
| Institutions | Beijing Jiaotong University, Dalian University of Technology |
Abstract
Section titled āAbstractāFollowing first principles and inspired by the special structure of the nickel-nitrogen color center, this work enhances the known diamond germanium-vacancy (GeV) color center by adding nitrogen (N) atoms and increasing the number of vacancies. Results demonstrate that the most stable structure is one without vacancies, where the germanium (Ge) atoms are connected to four N atoms. This work analyzes the new structure of the GeV color center and determines the charge transfer and bonding from the difference in charge density. The electron bands and density of states of the GeV color center with four N atoms are calculated. By analyzing the electrical properties of each atom, we posit that the N atom is a transitional modified atom. The new structure of the GeV color center has good prospects for use in sensors and single-photon sources.