A flexible nitrogen-vacancy center probe for scanning magnetometry
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2021-05-01 |
| Journal | Review of Scientific Instruments |
| Authors | Maosen Guo, Mengqi Wang, Pengfei Wang, Diguang Wu, Xiangyu Ye |
| Institutions | CAS Key Laboratory of Urban Pollutant Conversion, University of Science and Technology of China |
| Citations | 10 |
Abstract
Section titled āAbstractāThe key component of the scanning magnetometry based on nitrogen-vacancy centers is the diamond probe. Here, we designed and fabricated a new type of probe with an array of pillars on a (100 µm)2 Ć 50 µm diamond chip. The probe features high yield, convertibility to be a single pillar, and expedient reusability. Our fabrication is dramatically simplified by using ultraviolet laser cutting to shape the chip from a diamond substrate instead of additional lithography and time-consuming reactive ion etching. As an example, we demonstrate the imaging of a single magnetic skyrmion with nanoscale resolution. In the future, this flexible probe will be particularly well-suited for commercial applications.