Dual-color upconversion luminescence emission from Er -LiNbO3 on-chip ridge waveguides
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2021-07-07 |
| Journal | Results in Physics |
| Authors | Yuechen Jia, Yicun Yao, Shixiang Wang, Yingying Ren, Xingjuan Zhao |
| Institutions | Shandong Normal University, State Key Laboratory of Crystal Materials |
| Citations | 6 |
Abstract
Section titled āAbstractāDual-color upconversion luminescence of Er3+-doped (0.1% mol) lithium-niobate-on-insulator (Er:LNOI) on-chip ridge waveguides is observed under the excitation of a continuous-wave 980-nm semiconductor laser, emitting both blue (at 450 nm) and green (at 528.3 nm) fluorescence emissions. The on-chip waveguides, with a propagation loss of around 3 dB/cm at 1550 nm, are fabricated by diamond blade dicing technique. The experimentally observed waveguiding modal profiles are in fairly good agreement with simulation results, indicating good quality of the fabricated waveguides. We believe this work will benefit the development of LiNbO3-based integrated photonics.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2015 - Upconverting nanoparticles: a versatile platform for wide-field two-photon microscopy and multi-modal in vivo imaging [Crossref]
- 2018 - Advances in highly doped upconversion nanoparticles [Crossref]
- 2015 - Photochemical upconversion: present status and prospects for its application to solar energy conversion [Crossref]
- 2019 - Recent progress of rare-earth doped upconversion nanoparticles: synthesis, optimization, and applications [Crossref]
- 2007 - Resonant pumping and upconversion in 1.6 μm Er3+ lasers [Crossref]
- 2010 - Telecommunication-wavelength solid-state memory at the single photon level [Crossref]
- 2018 - Atomic source of single photons in the telecom band [Crossref]
- 2018 - Coherence time of over a second in a telecom-compatible quantum memory storage material [Crossref]
- 2006 - The past, present, and future of silicon photonics [Crossref]
- 2016 - Roadmap on silicon photonics [Crossref]