Study of the applicability of nano-polycrystalline diamond as a material for refractive x-ray lenses

MetadataDetails
Publication Date2021-09-21
AuthorsI. Snigireva, Tetsuo Irifune, Toru Shinmei, Polina Medvedskaya, Sergey Shevyrtalov
InstitutionsEhime University, Immanuel Kant Baltic Federal University
Citations3

The study of the applicability of a nano-polycrystalline diamond (NPD) as a lens material is presented. Two NPD plates with a diameter of 8 mm and a thickness of 0.1 and 1 mm were manufactured using the HPHT process. Coherence preservation properties of the NPD samples were checked using in-line phase-contrast imaging. Wide-Angle X-ray Scattering and Small Angle X-ray Scattering experiments were performed to examine the NPD scattering properties. Rotationally parabolic half-lens from a 100 μm thick NPD plate was manufactured using the maskless direct milling using a Zeiss CrossBeam 540 FIB-SEM system.