Determination of Copper and Iron in Real Sample of Water and Ethanol Using Square Wave Voltammetry with a Micro/Nano Boron-Doped Diamond Electrode

MetadataDetails
Publication Date2022-01-01
JournalMaterials Research
AuthorsAna Carolina dos Santos Ibernom, N.G. Ferreira, N.A. Braga
InstitutionsUniversidade Federal do Amazonas, National Institute for Space Research
Citations1

Abstract Currently, the search for a more economical alternative with adequate selectivity, sensitivity and reproducibility in the determination of metallic ions is important for the development of reliable methodologies for the determination of these contaminants. This work investigates a boron-doped micro/nano diamond electrode, with different morphology and structure compared to those discussed in the literature, for the detection of copper and iron in aqueous and ethanolic environments. Internal validation of the Square Wave Voltammetry was applied. The methodology was submitted to validation by: selectivity, linearity, precision (interday test), accuracy (percentage of recovery) and detection and quantification limits. The results indicated that this type of electrode showed good response to determinations in aqueous and ethanolic environments, with good selectivity, linearity, accuracy (recovery between 70% and 110%) and precision, presenting the best detection and quantification limits for the aqueous. The methodology using a boron-doped diamond micro/nano electrode was suitable for the determination of copper and iron metals in both matrices.

  1. 2021 - Recent advances of boron-doped diamond electrochemical sensors toward environmental applications
  2. 2021 - Recent developments of heavy metals detection in traditional Chinese medicine by atomic spectrometry
  3. 2021 - Study by absorption and emission spectrophotometry of the efficiency of the binary mixture (Ethanol-Water) on the extraction of betanin from red beetroot
  4. 2021 - A review on traditional uses, phytochemistry, pharmacology, toxicology and the analytical methods of the genus Nardostachys
  5. 2021 - Electrochemical evaluation of organic pollutant estradiol in industrial effluents [Crossref]
  6. 2021 - Antifouling lipid membrane coupled with silver nanoparticles for electrochemical detection of nucleic acids in biological fluids [Crossref]
  7. 2019 - Recent progress in the applications of boron doped diamond electrodes in electroanalysis of organic compounds and biomolecules - A review [Crossref]
  8. 2021 - Two extreme crystal size scales of diamonds, large single crystal and nanocrystal diamonds: Synthesis, properties and their mutual transformation [Crossref]
  9. 2017 - From micro to nanocrystalline boron doped diamond applied to cadmium detection [Crossref]
  10. 2020 - Performance parameters for analytical method validation: controversies and discrepancies among numerous guidelines [Crossref]