Composite Nitrogen-Vacancy Centers Nanodiamonds Grating using Soft Lithography
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2022-03-04 |
| Journal | 2022 Workshop on Recent Advances in Photonics (WRAP) |
| Authors | Rajesh Kumar, S. Anantha Ramakrishna |
| Institutions | Indian Institute of Technology Kanpur |
Abstract
Section titled āAbstractāComposite grating of Nitrogen-vacancy (N-V) centers nanodiamond (ND) is fabricated using soft lithography. Wide distribution with enhanced radiated powers from NDs is observed using confocal measurements. Numerical simulations reveal that this distribution arises from random emitting dipoles orientations inside the ND.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2010 - Soft lithography for micro-and nanoscale patterning [Crossref]
- 2017 - Nanoimprinted high-refractive index active photonic nanostructures based on quantum dots for visible light
- 2013 - Heterogeneous stacking of nanodot monolayers by dry pick-and-place transfer and its applications in quantum dot light-emitting diodes