Laminated wafer with conductive diamond layer formed by surface-activated bonding at room temperature for micro-electro mechanical system sensors
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2022-03-23 |
| Journal | Japanese Journal of Applied Physics |
| Authors | Yoshihiro Koga, Shunsuke Yamada, Shuji Tanaka, Kazunari Kurita |
| Institutions | Tohoku University, Sumco Corporation (Japan) |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Problem Solved: Replaces the insulating Buried Oxide (BOX) layer in Silicon-On-Insulator (SOI) wafers with a conductive boron-doped diamond layer to prevent plasma-induced charging during MEMS sensor fabrication.
- Alternative SOI Architecture: A laminated wafer (Si / BDD / Si) formed by Surface-Activated Bonding (SAB) at room temperature, eliminating the high-temperature (>800 °C) furnace oxidation step that contaminates conventional SOI wafers.
- Layer Specifications: Boron-doped diamond (BDD) layer deposited via MW-CVD with trimethoxyborane on a 2-inch Czochralski silicon base wafer.
- Key Material Properties: Resistivity of 0.025 Ω·cm (achieved at doping > 2 × 1021 atoms cm−3); polycrystalline grain size < 3 µm; selective etchability relative to silicon.
- Bonding Integrity: TEM confirmed no voids with gaps > 2 nm at the Si/diamond interface; only ~10 nm amorphous residue from Ar-ion bombardment.
- Cavity Formation: Diamond layer selectively etched by heat treatment in O2 atmosphere at ≥ 925 °C (etch rate ≥ 1 µm min−1), enabling cavity formation under the MEMS structure.
- Manufacturing Advantage: Lower metallic contamination, lower cost for small-batch/Specialty MEMS production, and compatibility with high-density plasma processes (RIE, PE-CVD, ashing).
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Base wafer material | (100) CZ-Si, P- or B-doped | — | 2-inch diameter, 3 mm thickness |
| Base wafer resistivity | 5 | Ω·cm | Doped Czochralski single crystal |
| Base wafer O2 concentration | 1.0-1.2 × 1018 | atoms cm−3 | Standard CZ spec |
| Bonding wafer material | (100) CZ-Si | — | 2-inch, 500 µm initial thickness |
| Bonding wafer post-grind thickness | 20 | µm | Silicon device layer |
| Diamond deposition method | MW-CVD (Nihon Koshuha MDD-2016) | — | MPCVD reactor |
| Deposition temperature | 1000 | °C | Substrate temp |
| Dopant precursor | Trimethoxyborane (B source) | — | In H2/CH4 carrier |
| Boron concentration (avg. 5 µm depth) | ~1.5 × 1021 | atoms cm−3 | SIMS analysis |
| Peak B concentration (surface) | ~6.4 × 1021 | atoms cm−3 | EELS line scan |
| Diamond layer thickness | 5-10 | µm | Tested |
| Diamond grain size | < 3 | µm | Polycrystalline |
| Diamond resistivity | 0.025 | Ω·cm | At ~2 × 1021 cm−3 B |
| Surface roughness post-polish | Ra < 1 | nm | Required for SAB |
| Bonding method | Surface-Activated Bonding (SAB) | — | Room temperature, UHV |
| Bonding vacuum | Ultrahigh vacuum | — | Short process time |
| Bonding interface void size | < 2 | nm | No defects detected |
| Amorphous layer thickness | 10 (2 × 5 nm) | nm | Residual from Ar-ion activation |
| Total laminated resistance (Rall) | ~1.5 | Ω | Dominated by base wafer |
| Diamond O2 etch threshold | 925 | °C | No etch at 920 °C / 30 min |
| Diamond O2 etch rate (≥ 925 °C) | ≥ 1 | µm min−1 | Heat treatment in O2 |
| Raman peak (diamond) | ~1332 | cm−1 | Confirms sp3 bonding |
Key Methodologies
Section titled “Key Methodologies”- Wafer Preparation: 2-inch (100) CZ-Si wafers (base: 3 mm; bonding: 500 µm) doped at resistivity 5 Ω·cm.
- Nanodiamond Seeding: Spin-coat nanodiamond/water solution; bake at 80 °C; seeding density > 106 cm−2.
- Diamond Deposition (MW-CVD): CH4 + trimethoxyborane + H2 at 1000 °C; deposit 5-10 µm polycrystalline BDD.
- Surface Polishing: Reduce diamond surface to Ra < 1 nm to meet SAB flatness requirements.
- Surface Activation (SAB): Ar-ion bombardment of both Si and diamond surfaces in UHV to generate dangling bonds.
- Bonding: Press Si wafer to BDD at room temperature in UHV; no voids > 2 nm detected by cross-sectional TEM.
- Backside Grinding: Reduce bonded Si wafer to 20 µm device layer.
- MEMS Fabrication: Pattern silicon nitride / photoresist; perform KOH trench etch through the Si device layer.
- Cavity Formation: Heat treatment in O2 at ≥ 925 °C fully removes the exposed diamond layer (≥ 1 µm min−1), releasing the MEMS structure.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials
Section titled “Applicable Materials”- Heavy Boron-Doped PCD (BDD): The paper specifies a resistivity of 0.025 Ω·cm at B concentrations exceeding 2 × 1021 atoms cm−3. 6CCVD’s heavy boron-doped polycrystalline diamond matches this specification and is the exact material class required to replicate or extend this research.
- Optional Optical-Grade SCD: For hybrid or next-generation device architectures requiring single-crystal diamond templates, 6CCVD supplies SCD substrates with Ra < 1 nm polish, suitable for direct bonding interfaces.
Customization Potential
Section titled “Customization Potential”- Wafer Dimensions: 6CCVD supports PCD plates up to 125 mm diameter and BDD thicknesses from 0.1 µm to 500 µm, covering the 5-10 µm range in the paper and beyond.
- Substrate Thickness: Base substrate thicknesses up to 10 mm are available for researchers needing thicker handle wafers.
- Metalization: If follow-on electrical characterization or contact integration requires patterned electrodes (e.g., Ti/Pt/Au for wire-bonding pads or surface passivation), 6CCVD offers in-house metalization with Au, Pt, Pd, Ti, W, and Cu.
- Laser Cutting & Dicing: Custom-shaped coupons and laser-cut geometries for 2-inch or smaller wafer experiments are available to bypass standard cleaving limitations.
- Surface Finish: In-house polishing ensures Ra < 5 nm on inch-size PCD and Ra < 1 nm on SCD, satisfying the strict flatness requirements of SAB.
Engineering Support
Section titled “Engineering Support”- 6CCVD’s in-house PhD-level engineering team can assist with material selection, doping concentration optimization, and surface preparation recipes for similar MEMS sensor, SOI replacement, and plasma-resistant wafer projects.
- Recommended stack for replication: BDD (5-10 µm, ~0.025 Ω·cm) on Si handle wafer, polished to Ra < 1 nm, ready for immediate SAB bonding trials.
Call to Action
Section titled “Call to Action”For custom specifications, BDD wafer fabrication, or material consultation on laminated wafer architectures, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Abstract We propose the use of a laminated wafer with a conductive diamond layer for forming cavities as an alternative silicon-on-insulator wafer for micro-electro mechanical system (MEMS) sensors. Since this wafer has no insulator such as a buried oxide (BOX) layer but a conductive layer, it is not charged during plasma treatment in MEMS sensor fabrication processes. The conductive diamond layer was formed on a base wafer doped with boron of more than 2 × 10 21 atoms cm −3 by microwave-plasma-enhanced chemical vapor deposition. The resistivity of this layer was 0.025 Ω cm, and this layer can be selectively etched to a base wafer made of silicon crystal, such as a BOX layer. In addition, a silicon wafer can be bonded to its layer without voids with gaps of more than 2 nm by surface-activated bonding. Therefore, we believe that the laminated wafer studied here is useful for the fabrication processes for MEMS sensors that may otherwise be damaged by plasma treatment.