Anomalous thermal response of bulk diamond to uniaxial (100) strain - A first-principles prediction
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2022-11-18 |
| Journal | Physical review. B./Physical review. B |
| Authors | Biao Wang, Jiwen Zhao, Yanwei Hu, Yurong He, N. B. Rodionov |
| Institutions | Troitsk Institute for Innovation and Fusion Research, Harbin Institute of Technology |
| Citations | 13 |
Abstract
Section titled āAbstractāDiamond, a material that exhibits ultrahigh thermal conductivity with a sensitive thermal response to stress, is an ideal heat-sink material in the embedded cooling paradigm. This study uses first-principles calculations with the phonon Boltzmann transport equation to predict the variation rules of the thermal conductivity of diamond along the $\ensuremath{\langle}100\ensuremath{\rangle}$ crystal direction under strains at three orders of magnitude: 0.1%, 1%, and 10.5%. Density functional theory is used to predict the stressāstrain dependence of diamond and the temperature-dependent thermal conductivity of unstrained diamond. The predictions are in good agreement with the experimental results. The calculated uniaxial straināthermal conductivity dependence results reveal that the thermal conductivity of diamond abnormally increases by approximately 15% under small-scale uniaxial strain because of the weakened anharmonic interatomic force constants. Under large-scale strain, the thermal conductivity considerably decreases because of reduced phonon group velocities and increased numbers of phonon scattering channels. The findings in this study will guide analyses of the dependence of thermal conductivity on strain in other diamondlike structures, such as Group IV element-based materials. The abnormal thermal response at small strain is expected to lead to the realization of an artificial thermal conduction channel.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2017 - IEEE International Conference on Microwaves, Antennas, Communications and Electronic Systems (COMCAS)