Formation of NV centers in diamond by a femtosecond laser single pulse
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2022-11-22 |
| Journal | Optics Express |
| Authors | Yasuhiko Shimotsuma, Keiko Kinouchi, Ryusei Yanoshita, Masanori Fujiwara, Norikazu Mizuochi |
| Institutions | Kyoto University, Kobe University |
| Citations | 12 |
Abstract
Section titled āAbstractāThe NV centers in a diamond were successfully created by the femtosecond laser single pulse. We also investigated the effect on the diamond lattice induced by the different laser pulse widths from both experimental and theoretical perspectives. Interestingly, in spite of the high thermal conductivity of a diamond, we found that there is a suitable pulse repetition rate of several tens kHz for the formation of NV center ensembles by the femtosecond laser pulse irradiation.