Skip to content

Evolution of local edge state braiding and spin topological transport characterization of Te-doped monolayer 1T′-MoS2

MetadataDetails
Publication Date2023-01-01
JournalPhysical Chemistry Chemical Physics
AuthorsQianjia Cheng, Zhengxin Yan, Wei Song, Juntao Kong, Dongxin Li
InstitutionsXi’an University of Science and Technology
Citations1

Our study explores spin transport in a MoS 1.75 Te 0.25 matrix, and find two types of fractional braidings in surface states: “diamond” and “tropical fish”, offering prospects for topological quantum computing.