High-resolution spectroscopy of a single nitrogen-vacancy defect at zero magnetic field
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2023-01-30 |
| Journal | Quantum Science and Technology |
| Authors | Shashank Kumar, Pralekh Dubey, Sudhan Bhadade, Jemish Naliyapara, Jayita Saha |
| Institutions | Indian Institute of Science Education and Research, Bhopal |
| Citations | 2 |
Abstract
Section titled āAbstractāAbstract We report a study of high-resolution microwave spectroscopy of nitrogen-vacancy (NV) centers in diamond crystals at and around zero magnetic field. We observe characteristic splitting and transition imbalance of the hyperfine transitions, which originate from level anti-crossings (LACs) in the presence of a transverse effective field. We use pulsed electron spin resonance spectroscopy to measure the zero-field spectral features of single NV centers for clearly resolving such LACs. To quantitatively analyze the magnetic resonance behavior of the hyperfine spin transitions in the presence of the effective field, we present a theoretical model, which describes the transition strengths under the action of an arbitrarily polarized microwave magnetic field. Our results are of importance for the optimization of the experimental conditions for the polarization-selective microwave excitation of spin-1 systems in zero or weak magnetic fields.