Green Diamond - A Superhard Boron Carbonitride with Bandgap in Green-Light Region and Anisotropic High Carrier Mobilities
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2023-03-31 |
| Journal | The Journal of Physical Chemistry Letters |
| Authors | Jiaqi Lin, Jiaxin Jiang, Jiaqi Zhang, Hongyan Guo, Xiao Cheng Zeng |
| Institutions | City University of Hong Kong, Anhui Normal University |
| Citations | 4 |
Abstract
Section titled āAbstractāThe development of new multifunctional superhard materials beyond diamond is a great challenge for materials science and industry application. A new diamond-like boron carbonitride material (BC<sub>6</sub>N) formed by covalently alternated stacking of two-dimensional BC<sub>3</sub> and C<sub>3</sub>N monolayers is systemically investigated through first-principles method. The electronic structure calculations show that the new structure is a direct bandgap semiconductor with a bandgap of 2.404 eV (HSE06). It exhibits anisotropic high carrier mobility (μ<sub><i>Lh</i></sub> = 1.88 Ć 10<sup>4</sup> cm<sup>2</sup> V<sup>-1</sup> s<sup>-1</sup>), varied absorbance in visible light and different regions of UV light, and theoretical Vickers hardness of 81.34 GPa, close to that of diamond. Furthermore, it is easily synthesizable due to its exothermic nature when reacted from the interlayer fusion of the BC<sub>3</sub> and C<sub>3</sub>N monolayers in a bottom-up synthesis strategy. In addition, the properties of 3D-BC<sub>6</sub>N-I can be tuned by applying strain, changing stacking patterns, and 2D-nanolization. The excellent mechanical, electronic, and optical properties and good synthesizability suggest that the new structure (named as āgreen diamondā) may find broad applications as a superhard and high-temperature material as well as a semiconductor and optical devices beyond diamond.