High quality GaN films on miscut (1 1 1) diamond substrates through non-c orientation suppression
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2023-03-20 |
| Journal | Results in Physics |
| Authors | Yuan Gao, Shengrui Xu, Hongchang Tao, Yachao Zhang, Jinfeng Zhang |
| Institutions | Xidian University |
| Citations | 4 |
Abstract
Section titled âAbstractâThe GaN films are grown on 4° miscut to (110) and (100) orientation (111) diamond substrates by metal organic chemical vapor deposition respectively. The ordinary (111) diamond substrate is used as reference. The morphology and crystal quality of the three GaN films are characterized by atomic force microscope, scanning electron microscope, Raman spectra, photoluminescence, and X-ray diffraction (XRD). The GaN epilayer on miscut to (110) orientation (111) diamond presents a superior quality with smooth surface, clear A1(LO) peak of Raman shift and XRD rocking curve with full width half maximum of 1357 arcsec, which is a remarkable result reported. Through the analysis, we found that when GaN grows on miscut to (110) orientation (111) diamond substrates, non-c orientation grain would be greatly suppressed so that c orientation buffers easier to grow laterally and merge into thin films. The non-c orientation suppression process greatly improves the quality of GaN film on (111) diamond.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2019 - Characterization and optimization of MIS-HEMTs device of highâźk dielectric material on quaternary barrier of Al0.42ln0.03Ga0.55N/UID-AIN/GaN/GaN heterostructure for high power switching application
- 2018 - Thermal characterization of gallium nitride p-i-n diodes [Crossref]
- 2018 - Nearly-zero valence band and large conduction band offset at BAlN/GaN heterointerface for optical and power device application [Crossref]
- 2014 - Self-Heating in GaN Transistors Designed for High-Power Operation [Crossref]
- 1998 - Self-Heating in High-Power AlGaN-GaN HFETâs [Crossref]
- 2015 - Reduction of leakage current by O2 plasma treatment for device isolation of AlGaN/GaN heterojunction field-effect transistors [Crossref]
- 2015 - Reducing GaN-on-diamond interfacial thermal resistance for high power transistor applications [Crossref]
- 2010 - Formation and characterization of 4-inch GaN-on-diamond substrates [Crossref]
- 2011 - AlGaN/GaN high-electron mobility transistors with low thermal resistance grown on single-crystal diamond (111) substrates by metalorganic vapor-phase epitaxy [Crossref]