Anisotropic thermal property characterizations and optical phonon contribution analysis of ZnO under high pressure

MetadataDetails
Publication Date2023-04-20
JournalJournal of Materials Research and Technology
AuthorsXuanhui Fan, Zhongyin Zhang, Jing Zhou, Kunpeng Yuan, Jie Zhu
InstitutionsDalian University of Technology
Citations6

Zinc oxide (ZnO) is a wide band-gap semiconductor material with versatile applications in high-tech fields. Under high pressure, ZnO exhibits multiple phase transitions, which are of great significance for the development of photocatalysts, micro-devices with stress-controlled elements, and the investigation of relevant structure-activity relationships. However, previous studies have reported only theoretical calculations of its thermal transport properties under high pressure due to the challenges of experimental methodology. In this work, we employed a combination of the time-domain thermoreflectance technique and diamond anvil cell to characterize the anisotropic thermal properties of ZnO crystal under 0-20 GPa. Simultaneously, we studied the micro-structure of ZnO in the same pressure range by Raman spectra. Our proposed modified Leibfried-Schlomann equation adequately explained the non-monotonic trend of the thermal conductivity within 10 GPa observed in measurement results. Additionally, we report the ZnO thermal conductivity during the decompression process for the first time. Our experimental results and theoretical analysis advance the understanding of the thermal transport mechanism of wide-gap semiconductors under high pressure and pave the way for their high-pressure modification.

  1. 2019 - ZnO as a functional material, a review [Crossref]
  2. 2008 - Electrically pumped ultraviolet ZnO diode lasers on Si [Crossref]
  3. 2010 - ZnO nanoparticle surface acoustic wave UV sensor [Crossref]
  4. 2009 - Solution-processed zinc oxide transistors for low-cost electronics applications [Crossref]
  5. 2012 - Surface acoustic wave hydrogen sensors based on ZnO nanoparticles incorporated with a Pt catalyst [Crossref]
  6. 2018 - Light-soaking free organic photovoltaic devices with sol-gel deposited ZnO and AZO electron transport layers [Crossref]
  7. 2003 - Thin-film transistor fabricated in single-crystalline transparent oxide semiconductor [Crossref]
  8. 2017 - Materials discovery at high pressures
  9. 2002 - New materials from high-pressure experiments [Crossref]
  10. 1996 - High-pressure synthesis of high-purity diamond crystal [Crossref]