Skip to content

Silicon Vacancy in Boron-Doped Nanodiamonds for Optical Temperature Sensing

MetadataDetails
Publication Date2023-08-30
JournalMaterials
AuthorsMasfer Alkahtani
InstitutionsKing Abdulaziz City for Science and Technology
Citations6

Boron-doped nanodiamonds (BNDs) have recently shown a promising potential in hyperthermia and thermoablation therapy, especially in heating tumor cells. To remotely monitor eigen temperature during such operations, diamond color centers have shown a sensitive optical temperature sensing. Nitrogen-vacancy (NV) color center in diamonds have shown the best sensitivity in nanothermometry; however, spin manipulation of the NV center with green laser and microwave-frequency excitations is still a huge challenge for biological applications. Silicon-vacancy (SiV) color center in nano/bulk diamonds has shown a great potential to be a good replacement of the NV center in diamond as it can be excited and detected within the biological transparency window and its thermometry operations depends only on its zero-phonon line (ZPL) shift as a function of temperature changes. In this work, BNDs were carefully etched on smooth diamond nanocrystals’ sharp edges and implanted with silicon for optical temperature sensing. Optical temperature sensing using SiV color centers in BNDs was performed over a small range of temperature within the biological temperature window (296-308 K) with an excellent sensitivity of 0.2 K in 10 s integration time. These results indicate that there are likely to be better application of more biocompatible BNDs in hyperthermia and thermoablation therapy using a biocompatible diamond color center.

  1. 2020 - Experimental demonstration of memory-enhanced quantum communication [Crossref]
  2. 2018 - Photon-mediated interactions between quantum emitters in a diamond nanocavity [Crossref]
  3. 2011 - Diamond photonics [Crossref]
  4. 2019 - Nanodiamond Integration with Photonic Devices [Crossref]
  5. 2018 - Fluorescent nanodiamonds: Past, present, and future [Crossref]
  6. 2013 - Tracking the engraftment and regenerative capabilities of transplanted lung stem cells using fluorescent nanodiamonds [Crossref]
  7. 2016 - Diamond Quantum Devices in Biology [Crossref]
  8. 2023 - Engineering sub-10 nm fluorescent nanodiamonds for quantum enhanced biosensing [Crossref]
  9. 2020 - Boron-Doped Nanodiamonds as Anticancer Agents: En Route to Hyperthermia/Thermoablation Therapy [Crossref]