Skip to content

RESEARCH OF THERMAL INFLUENCE ON THE CHANGE OF THE SURFACE LAYER OF DIAMONDS AND ASSOCIATED TOOL MATERIALS (REVIEW)

MetadataDetails
Publication Date2023-12-25
JournalCollection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
AuthorsV. I. Lavrinenko, Volodymyr Solod, Ilnytska Halina, V. V. Smokvyna, Kashynskiy Ivan
InstitutionsV. Bakul Institute for Superhard Materials, Dniprovsk State Technical University
Citations1
AnalysisFull AI Review Included

Thermal Effects on Diamond Surface Engineering: Interface Coatings & Tool Optimization

Section titled “Thermal Effects on Diamond Surface Engineering: Interface Coatings & Tool Optimization”
  • Domain: Review of 2023 advances in thermal interactions at diamond and tool-material interfaces, emphasizing surface modification, doping, and protective coatings.
  • Core Finding - Graphitization: Adsorbed Fe and W adatoms destabilize the C-C interlayer bonding on diamond (110) and (111) surfaces, inducing surface graphitization, which directly impacts wear and adhesion behavior in metal-bond grinding systems.
  • Coating Strategies: Multilayer nitride architectures (cBN/NCD, AlN/diamond nanopillars, TiSiN/AlCrN, Ti(C,N)-Al2O3) outperform monolayer systems under thermal load by reducing thermal boundary resistance (TBR) up to 28% and improving tribological stability.
  • Surface Termination Engineering: High-voltage hydroxide treatment (up to 3000 V) produces OH-diamond surfaces exhibiting enhanced oxidation resistance, while H-terminated diamond(111)/h-BN heterostructures show improved charge transfer and hole accumulation.
  • Multi-Doping for Oxidation Resistance: B, N, and Si multi-doped diamond films display the highest activation energy among doped models, providing a pathway to oxidation-resistant CVD diamond for high-temperature tooling.
  • Cemented Carbide Tool Insight: Dry finish-milling of compacted graphite iron (CGI) reveals (Fex,W1-x)3C phase formation at WC-Co interfaces, accelerating flank wear — highlighting the need for thermally stable diamond coatings on tool substrates.
  • Practical Implication: Rough-surface CVD diamond demonstrates superior adhesion in Ni-diamond electrodeposited composites (microhardness up to 613 HV, friction coefficient reduced to 0.63, wear rate decreased by 15.6%).
ParameterValueUnitContext / Source
Oxidative etching temperature range600 - 900°CSynthetic diamond microcrystals, Ref. [6]
Etch conversion threshold (skeletal type)High conversion < 700°C{111} facet selective etching, Ref. [6]
Anti-skeletal formation temperature900°C30-50% transformation, Ref. [6]
Hydroxide ion treatment voltageup to 3000VOH-diamond fabrication, Ref. [13]
Ni-diamond composite microhardness613HVRough-surface diamond coating #3, Ref. [15]
Friction coefficient (Ni-diamond #3)0.63-vs. standard Ni-diamond, Ref. [15]
Wear rate reduction15.6%Composite coating #3 vs. reference, Ref. [15]
Cr-CVD diamond S/S reaction temperature500 - 600°CDominant Cr23C6 phase, Ref. [16]
AlN/diamond TBR reduction (nanopillars)28%vs. planar interface, Ref. [18]
hBN twist-induced vdW enhancementTunable-H-diamond(111)/hBN heterostructure, Ref. [19]
Workpiece materialEN-GJV-450 CGI (90-95% perlite)-Dry finish milling, Ref. [24]
Cutting speed vc150m/minCemented carbide tool wear, Ref. [24]
Coating architecture testedTi(C,N)-Al2O3 multilayer-CVD coating, Ref. [24]
Tribolayer identifiedTi-oxide-TiSiN/AlCrN system, Ref. [22]
Dominant wear mechanism (high-T)Oxidative (not abrasive)-TiSiN/AlCrN PVD coating, Ref. [22]
Interfacial carbide phase(Fex,W1-x)3C-WC-Co + CGI interaction, Ref. [24]
  • Surface Oxidation Studies (Ref. [6]): Synthetic diamond microcrystals subjected to controlled oxidative etching in O2/air across 600-900 °C; morphology tracked via SEM to map {111}/{100} etch pit evolution.
  • First-Principles DFT Modeling (Ref. [10], [11]): Adsorption of Fe and W adatoms on diamond (110) and (111) surfaces simulated to evaluate interlayer C-C bond weakening and graphitization energetics.
  • Multi-Doped CVD Diamond Growth (Ref. [12]): B, N, and Si co-doping during CVD diamond film deposition; activation energies computed and validated against oxidation experiments.
  • High-Voltage OH-Termination (Ref. [13]): Diamond substrates immersed in deionized water with hydroxide ions, biased up to 3000 V, producing stable C-OH and C-O-C surface groups.
  • Electrodeposited Ni-Diamond Composites (Ref. [15]): Diamond grit surface roughened prior to Ni co-deposition; microhardness, friction coefficient, and wear rate quantified against smooth-diamond controls.
  • Solid-State Cr-Diamond Interface Analysis (Ref. [16]): Sputtered Cr films on CVD diamond (100) annealed at 500-600 °C; XPS and TEM used to identify early-stage disordered carbon and carbide phase formation.
  • Molecular Dynamics Interface Engineering (Ref. [18]): AlN/diamond nanopillar arrays modeled to minimize thermal boundary resistance compared to planar interfaces.
  • Twist-Angle Heterostructure Assembly (Ref. [19]): H-terminated diamond(111) coupled to hBN at varied twist angles; electronic band alignment and charge transfer characterized.
  • CVD Multilayer Tool Testing (Ref. [24]): Ti(C,N)-Al2O3 coated cemented carbide inserts run in dry finish milling of CGI; tool degradation tracked at 5%, 10%, 25%, and 100% of tool life.
  • PVD Coating Tribometry (Ref. [22]): TiSiN/AlCrN coatings evaluated across temperature regimes; Raman spectroscopy identified Ti-oxide tribolayer formation.
Paper RequirementRecommended 6CCVD Material
CVD diamond films for graphitization/oxidation studiesOptical Grade SCD (single crystal, ultra-low defect density)
Cr-sputtered diamond interface reactionsStandard PCD wafers (up to 125 mm, polished Ra < 5 nm)
OH-/H-terminated diamond surface studiesSCD plates with custom polishing (Ra < 1 nm) for controlled termination chemistry
B/N/Si multi-doped oxidation-resistant filmsHeavy Boron-Doped Diamond (BDD) or custom-doped PCD
Rough-surface diamond for Ni composite adhesionPCD with engineered surface morphology (custom laser texturing)
AlN/diamond thermal interface structuresPCD substrates (up to 10 mm thickness) suitable for epitaxial or sputtered nitride stacks
Ti(C,N)-Al2O3 coated carbide tool studiesPCD cutting tool blanks with custom edge preparation
  • Metalization: The review highlights Cr sputtering, Ni electrodeposition, and Ti-based multilayer coatings on diamond. 6CCVD provides in-house Au, Pt, Pd, Ti, W, and Cu metalization with precise thickness control, enabling direct replication of Cr-diamond S/S interface studies and Ni-diamond composite work without third-party processing delays.
  • Dimensional Flexibility: Custom SCD and PCD thicknesses from 0.1 µm to 500 µm accommodate thin-film graphitization studies (Ref. [10], [11]) as well as bulk substrate work for AlN/diamond TBR experiments (Ref. [18]).
  • Laser Cutting & Shaping: Rough-surface diamond composites (Ref. [15]) and nanopillar-engineered interfaces (Ref. [18]) benefit from precision laser cutting, available in-house to deliver application-specific geometries.
  • Surface Finishing: Polishing capabilities down to Ra < 1 nm (SCD) and Ra < 5 nm (inch-size PCD) support the clean-surface baselines required for XPS, XANES, and EXAFS characterization referenced throughout the review.
  • The paper’s emphasis on hBN/diamond heterostructures (Ref. [19]), multi-doped CVD diamond oxidation resistance (Ref. [12]), and thermal boundary resistance reduction (Ref. [18]) represents frontier work where material purity, dopant uniformity, and interface quality are critical. 6CCVD’s in-house PhD engineering team can advise on:
    • Selecting between SCD and PCD for specific termination chemistry protocols.
    • Matching diamond grade (optical, thermal, mechanical) to the experiment’s dominant failure mode — graphitization, oxidation, or adhesive wear.
    • Co-designing metalization stacks (e.g., Ti/Pt/Au) compatible with subsequent sputtering or electrodeposition steps described in the review.
  • For projects targeting tool-life extension in CGI machining (Ref. [24]) or self-lubricating coated tools (Ref. [14]), 6CCVD can supply PCD grades optimized for thermal stability and interfacial compatibility with Ti(C,N)-Al2O3 CVD coatings.

For custom specifications, doped diamond formulations, metalization stack design, or material consultation on thermal-interface and tool-wear research, visit 6ccvd.com or contact the 6CCVD engineering team directly. Global shipping available (DDU default; DDP on request).

View Original Abstract

Attention is drawn to the fact that the issues of effective processing of such fragile, difficult-to-process materials as mono- and polycrystalline diamonds are currently being discussed in the literature, including CVD diamond films, sapphire, etc. For the most part, such processing is faced with the issues of thermal impact on the surface of the tool material, taking into account the defects of the diamonds that undergo processing, directed impact on the surface of such diamonds, heat and modification of the surface of diamonds and accompanying tool materials.
 In this review, attention is focused on the newest modern developments, namely 2023, in the features of thermal effects on carbon materials, diamond, and steel. Studies are shown in the direction of directed changes in the surface of diamonds: obtaining the surface of OH-diamonds and H-diamonds, doping diamond, and changing the contact of the diamond surface with Fe and W. Special attention is paid to the application of various protective coatings on the surface of diamonds and related tool materials (steels, ceramics and hard alloys). At the same time, the greatest attention is paid to metal and nitride coatings, that is, this direction has recently become important and relevant.
 Various models of doped diamond, places of adsorption of O atoms on its various surfaces, and the subsequent process of the reaction of the O2 molecule with the C atom are considered. The results show that the multi-alloy diamond model has the highest activation energy, which reflects the best properties of oxidation resistance. Research shows that diamond with a rough surface has a larger surface area and higher electronegativity than normal diamond, which improves the adhesion between the Ni-based bond and the diamond with a rough surface.