Skip to content

Synthesis of gold nanoparticles with allicin to modify boron-doped diamond surface for oxygen sensor applications

MetadataDetails
Publication Date2023-12-31
JournalEnvironmental and Materials
AuthorsToto Raharto, Cahya Mukti Setiyanto, Harits Atika Ariyanta, Dinda P. N. Nahda, Adinda Muthia Hani
InstitutionsGunadarma University, University of Indonesia
AnalysisFull AI Review Included
  • Objective: Fabrication of a highly sensitive electrochemical dissolved oxygen (DO) sensor using a Boron-Doped Diamond (BDD) electrode modified with green-synthesized gold nanoparticles (AuNPs).
  • Core Innovation: Utilization of allicin (extracted from garlic via salting-out) as a bio-capping/reducing agent for AuNP synthesis, followed by UV-assisted photoreduction deposition onto the BDD surface.
  • Material Verification: Raman spectroscopy confirmed high sp3/diamond phase purity with no detectable sp2 carbon impurities near ~1500 cm-1.
  • Analytical Performance: Achieved a Limit of Detection (LOD) of 0.12 ppm and Limit of Quantification (LOQ) of 0.41 ppm for dissolved oxygen in 0.1 M PBS (pH 7).
  • Sensitivity & Stability: Demonstrated a high sensitivity of -19.086 µA/ppm with excellent reproducibility (%RSD = 6.86 over 6 repeated measurements).
  • Methodology: Three-electrode cyclic voltammetry system (AuNPs-BDD working, Ag/AgCl reference, Pt wire counter) sweeping from -1.0 V to +1.5 V.
  • Gold Coverage: Optimized AuNP surface coverage on the BDD substrate measured at 0.6% (w/w).
ParameterValueUnitContext
BDD Cleaning10minUltrasonication in 2-propanol + water
AuNP ReactantHAuCl4·4H2O0.01 % (w/v)Gold precursor solution
Allicin Concentration Range0.01 - 0.1% (v/v)Capping agent concentration gradient
Reducing AgentNaBH4 (0.1 M)0.5 mLUsed for gold ion reduction
UV Irradiation Power100WPower source for AuNP-BDD modification
UV Deposition Time6hDuration of BDD surface functionalization
Electrolyte0.1 M PBSpH 7Supporting electrolyte for CV
Potential Window-1.0 to +1.5VCyclic voltammetry scan range
Reference ElectrodeAg/AgCl—Standard reference half-cell
Counter ElectrodePt wire—Auxiliary electrode material
AuNP Surface Coverage0.6% (w/w)Final deposition on BDD
Limit of Detection (LOD)0.12ppmDissolved oxygen detection
Limit of Quantification (LOQ)0.41ppmDissolved oxygen quantification
Sensitivity-19.086µA/ppmElectrochemical response slope
Reproducibility (%RSD)6.86%Across 6 measurement cycles
Linear Regression (CV)y = -4.579x + 19.086—Current vs. concentration fit (R2 = 0.9986)
  • Substrate Preparation: BDD films cleaned via sequential ultrasonication in 2-propanol (10 min) and ultrapure water to remove surface contaminants prior to modification.
  • Allicin Isolation: Garlic cloves ground into powder, ultrasonic-assisted extraction in absolute ethanol (20 min), followed by salting-out extraction using 23% (w/w) ammonium sulfate and 24% (w/w) ethanol.
  • AuNP Green Synthesis: Mixing 5 mL of 0.01% (w/v) HAuCl4·4H2O with varying allicin concentrations (0.01-0.1% v/v), followed by addition of 0.5 mL 0.1 M NaBH4; reaction confirmed by yellow-to-red wine color change.
  • Surface Modification: Immersion of BDD films in AuNP colloidal solution under 100 W UV light for 6 hours to photodeposit the nanoparticles onto the diamond surface.
  • Electrochemical Evaluation: Cyclic voltammetry executed in a standard three-electrode cell against an Ag/AgCl reference, scanning from -1.0 V to +1.5 V in oxygenated 0.1 M PBS (pH 7).
  • Applicable Materials:
    • This research relies on a highly conductive, sp3-pure diamond substrate. 6CCVD’s Heavy Boron-Doped Polycrystalline Diamond (BDD) is the direct material match for replicating this sensor architecture. Our MPCVD-grown BDD ensures the low background current, wide electrochemical window, and phase purity required for sub-ppm oxygen detection.
  • Customization Potential:
    • The study utilized a bare BDD film modified via wet-chemistry deposition. For scaled sensor production, 6CCVD provides in-house metallization (Ti, Au, Pt, Pd, W, Cu) to create patterned or full-area electrical contacts, eliminating the need for external conductive epoxies.
    • We support custom dimensions including plates/wafers up to 125 mm, allowing direct integration into microfluidic or multi-electrode sensor arrays.
    • Our laser cutting and polishing services (Ra < 5 nm for inch-size PCD) enable precise electrode geometries and surface finishes to optimize AuNP adhesion kinetics.
  • Engineering Support:
    • Replicating or extending this DO/BOD sensor platform requires tight control over boron concentration and surface sp2/sp3 ratio. 6CCVD’s in-house PhD engineering team can collaborate on material selection, doping levels, and surface termination to fine-tune electron transfer kinetics for novel biosensor and environmental monitoring projects.
    • Whether the application is dissolved oxygen sensing, BOD analysis, or broader electrochemical detection, our team provides end-to-end consultation from substrate specification to metallization stack design.
  • Call to Action:
    • For custom specifications, tailored boron-doping concentrations, or material consultation for your sensor development, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract

Modification of surface of boron-doped diamond (BDD) film with gold nanoparticles (AuNPs) was carried out to increase its catalytic activity for an application as an oxygen sensor. Allicin was isolated from garlic by salting out extraction technique, and then used as the capping agent to synthesize AuNPs as it has a double bond structure that could be reacted to attach the BDD surface under UV light radiation. An average size of AuNPs at around 46,00 ± 9,06 nm was obtained, while the modification of the BDD surface by the synthesized AuNPs indicated that the surface of BDD could be covered by gold at around 0.6 % (w/w). Investigation of the AuNPs-modified BDD as a working electrode for the oxygen reduction by using cyclic voltammograms in 0.1 M phosphate buffer solution pH 7 observed a current peak at around -0.45 V (vs. Ag/AgCl). The current of this peak linearly increased proportionally to the dissolved oxygen concentrations (R2=0.9986). Moreover, a limit of detection of the dissolved oxygen of 0.12 ppm and limit of quantity 0.41 ppm could be achieved with excellent stability at 6.86% RSD with 6 repetitions and sensitivity at 19.086 μA/ppm indicated that the modified BDD is promising for applications as an oxygen sensor.