A chemical coating strategy for assembling a boron-doped diamond anode towards electrocatalytic degradation of late landfill leachate
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2024-01-01 |
| Journal | RSC Advances |
| Authors | Juanmei Zeng, Xi Liu, Qizhi Chen, Dongying Hu |
| Institutions | Guangxi University |
| Citations | 4 |
Abstract
Section titled âAbstractâA chemical coating strategy for assembling boron-doped diamond anode towards electrocatalytic degradation of late landfill leachate with high removal rates of organic carbon (TOC) and ammonia nitrogen after electrochemical oxidation.