Vertically aligned boron-doped diamond nanostructures as highly efficient electrodes for electrochemical supercapacitors

MetadataDetails
Publication Date2024-01-01
JournalJournal of Materials Chemistry A
AuthorsShradha Suman, Dhananjay K. Sharma, Ondrej Szabó, Benadict Rakesh, MariÔn Marton
InstitutionsAcademy of Scientific and Innovative Research, Czech Academy of Sciences, Institute of Physics
Citations8

Nanostructuring boron-doped diamond effectively improves the electrochemical supercapacitor performance with high lifetime stability.