Abstract
Section titled âAbstractâAbstract The design of efficient single-atom catalysts (SACs) with optimal activity and selectivity for sustainable energy and environmental applications remains a challenge. In this work, comprehensive first-principles calculations are performed to validate the feasibility of single TM atoms ( 3d , 4d , and 5d series) embedded in two different conformations of graphitic carbon nitride (g-C 3 N 4 ) monolayers. Additionally, we investigate the effect of nitrogen vacancies in the g-C 3 N 4 monolayers on the absorption of SACs considering three potential absorption scenarios that correspond to different experimental conditions. Our results point to the most stable configurations with the lowest formation energies and indicate that the absorption of single TM atoms on-vacancy and on-center sites are more favorable than via-substitution. In addition to the thermodynamic stability, electrochemical stability is also investigated through the calculation of the dissolution potential of the SACs. Within the scenarios considered in this study, we find that Pt, Pd, Rh, Au, Ru, Ir, Cu, Co, Fe, and Ni will produce the most robust SACs on both (edge and bridge) N vacancy site of reduced g-C 3 N 4 . Our findings provide guidance for the design and development of g-C 3 N 4 sheets decorated with single TM atoms for technological applications such as pollutant degradation, CO 2 reduction, N 2 fixation, selective oxidation, water splitting, and metal ion-based batteries.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2020 - Single-atom catalysts across the periodic table [Crossref]
- 2020 - Theoretical insights into single-atom catalysts [Crossref]
- 2020 - Single-atom site catalysts for environmental catalysis [Crossref]
- 2018 - Single-atom catalysts for the hydrogen evolution reaction [Crossref]
- 2021 - Coordination engineering of single-atom catalysts for the oxygen reduction reaction: a review [Crossref]
- 2021 - Recent advances in strategies for improving the performance of CO2 reduction reaction on single atom catalysts [Crossref]
- 2021 - Single atom catalysts for fuel cells and rechargeable batteries: principles, advances, and opportunities [Crossref]
- 2023 - Modelling single atom catalysts for water splitting and fuel cells: a tutorial review [Crossref]
- 2022 - Advances in the development of single-atom catalysts for high-energy-density lithium-sulfur batteries [Crossref]